Pre-Treatment Methods for Vintage Balsa?

Collapse
X
 
  • Time
  • Show
Clear All
new posts
  • Earl
    Apollo Nut
    • Dec 2006
    • 6865

    #1

    Pre-Treatment Methods for Vintage Balsa?

    I build mostly old vintage kits (at the slow pace I can work on models) and at times I have challenges filling balsa grain on vintage nocecones and fins. I get them filled, but that old balsa seems to soak up a lot of filler coat and/or primer.

    Like a lot of builders, the filling and sanding steps are not my favorite pastime, but it seems to be made even more tedious with these vintage balsa pieces. I have an Estes Omega that I am getting ready for final paint, and I got those fins filled ok, but it seemed to take many more coats of filler and primer to get the fin grain properly smooth and grain-free.

    I'm maybe overly picky about filling all the grain in balsa, but I like to make these vintage builds really look as much like their catalog counterparts that I drooled over as a kid.

    Any techniques or secrets out there that others have tried that seem to work better with this old, parched balsa?

    Thanks,

    Earl
    Earl L. Cagle, Jr.
    NAR# 29523
    TRA# 962
    SAM# 73
    Owner/Producer
    Point 39 Productions

    Rocket-Brained Since 1970
  • sandman
    Custom Cone, Kit & Decal Maker
    • Mar 2005
    • 5082
    • Way North of Detroit

    #2
    Originally posted by Earl
    I build mostly old vintage kits (at the slow pace I can work on models) and at times I have challenges filling balsa grain on vintage nocecones and fins. I get them filled, but that old balsa seems to soak up a lot of filler coat and/or primer.

    Like a lot of builders, the filling and sanding steps are not my favorite pastime, but it seems to be made even more tedious with these vintage balsa pieces. I have an Estes Omega that I am getting ready for final paint, and I got those fins filled ok, but it seemed to take many more coats of filler and primer to get the fin grain properly smooth and grain-free.

    I'm maybe overly picky about filling all the grain in balsa, but I like to make these vintage builds really look as much like their catalog counterparts that I drooled over as a kid.

    Any techniques or secrets out there that others have tried that seem to work better with this old, parched balsa?

    Thanks,

    Earl
    After sanding to shape, glue the fins on, coat the wood (both sides at once) with Elmer's white glue straight out of the bottle.

    Wait a few hours and sand with 220 grit then use filler.
    The wood won't take quite as much sealer and primer.
    "I'm a sandman. I've never killed anyone. I terminate runners when their time is up." Logan from "Logan's Run"

    http://sandmandecals.com/

    Comment

    • astronwolf
      Lost his Drifter
      • Mar 2013
      • 1796
      • Northeast Ohio

      #3
      Originally posted by Earl
      I'm maybe overly picky about filling all the grain in balsa, but I like to make these vintage builds really look as much like their catalog counterparts that I drooled over as a kid.
      Earl. I am in a real building mode with balsa and cardboard oldie clones. I am setting the old vintage balsa aside, but the task of filling SO MANY balsa cones and fins with dope has turned into more of a chore than a leisure pastime.

      At first, I tried a more purist approach and stuck with dope, but that got real old. I am building about 9+ oldies all at once, and it turned into a lot of work. Now I use Elmers Exterior Wood Filler, like the old Fill 'n Finish, diluted with water to toothpaste consistency. I paint that stuff on, wipe off the excess, and I'm basically done. Depending on the consistency of the mix, it can be a one shot, wipe on once and you're done, coating. I sand down the filler, give it a shot of Deft Lacquer Sealer, and it's almost done. The Deft product really lets me know if I am smooth enough depending on how flat it lies on the part. Ideally I'd hit it with some sort of high build primer, but I can't do that until it warms up outside. The Deft or Primer let's me see any irregularities that I have left to take care of after the Fill 'n Finish.

      This has been the least arduous approach for me. Just wipe that diluted Elmers stuff on, and use primer to see what's left to fill. Sand the primer down. My very basic technique is nothing I invented, and it helped me take fourth (third if I didn't get ripped with someone's lame 'misson points') in the Scale event at NARAM-55.

      Good luck. Building is fun. Painting is fun. Surface prep can be a drag. Try what I suggest and see if doesn't help.
      -Wolfram v. Kiparski
      NAR 28643 - TRA 15520
      MTMA Section #606 President

      Comment

      • Earl
        Apollo Nut
        • Dec 2006
        • 6865

        #4
        Guys -

        Thanks for the two suggestions.....will hope to try them both and see how they do.

        I knew someone on this forum had probably come across the same problem before and had some kind of a workaround.

        On both Elmer's suggestion (especially the straight brush on glue solution) ever have any issues with warpageon on fins from the water in the Elmer's?


        Thanks again,

        Earl
        Earl L. Cagle, Jr.
        NAR# 29523
        TRA# 962
        SAM# 73
        Owner/Producer
        Point 39 Productions

        Rocket-Brained Since 1970

        Comment

        • CPMcGraw
          In Memoriam
          • Mar 2005
          • 5357
          • Mobile, Alabama

          #5
          Third suggestion, and it works well...

          Self-adhesive label paper. I've used it now for several years with no de-laminating issues. You apply it to the fin, trim it to shape, seal the outer edges with thin CA, give it a light sanding to eliminate the CA jaggies, and you're ready for the primer. Just keep the CA away from the root edge, of course...

          This method works well for balsa in almost any condition, short of dissolving in your hands if you breathe on them. It creates a 'composite' structure, like plywood.

          Alternate method would be plain paper, with a spray of 3M-77, or 3M-90 contact adhesive to attach it.

          IIRC, even Estes sold sheets of sticky-back paper in their parts section of the catalogs of the late '60s, just for this purpose. If you're looking for something that is in keeping with the old traditions, consider that Estes was promoting this method 45 years ago...
          Craig McGraw

          BARCLONE Rocketry -- http://barclone.rocketshoppe.com
          BARCLONE Blogsite -- http://barclone.wordpress.com
          BARCLONE Forum -- BARCLONE Forum

          BARs helping BARs

          SAM 0044
          AMA 352635

          Comment

          • sandman
            Custom Cone, Kit & Decal Maker
            • Mar 2005
            • 5082
            • Way North of Detroit

            #6
            Originally posted by Earl
            Guys -

            Thanks for the two suggestions.....will hope to try them both and see how they do.

            I knew someone on this forum had probably come across the same problem before and had some kind of a workaround.

            On both Elmer's suggestion (especially the straight brush on glue solution) ever have any issues with warpageon on fins from the water in the Elmer's?


            Thanks again,

            Earl
            I've never run into a warpage problem yet and I've been doing it this way since the early sixties.

            Just be sure the fin is glued onto the body tube securely first.

            The white glue seals the wood and prevents the wood from "soaking up" the filler and primer.

            Not sure but I think the glue surface helps the primer/paint adhere to the wood better.

            White glue is cheap, non toxic, it won't glue your skin together and cleans up with water.
            "I'm a sandman. I've never killed anyone. I terminate runners when their time is up." Logan from "Logan's Run"

            http://sandmandecals.com/

            Comment

            • Bill
              I do not like Facebook
              • Sep 2008
              • 4107
              • North Tejas

              #7
              Originally posted by Earl
              On both Elmer's suggestion (especially the straight brush on glue solution) ever have any issues with warpageon on fins from the water in the Elmer's?


              Do both sides of the fin in one sitting instead of do one side, let it dry, then do the other side.


              Bill
              It is well past time to Drill, Baby, Drill!

              If your June, July, August and September was like this, you might just hate summer too...

              Please unload your question before you ask it unless you have a concealed harry permit.

              : countdown begin cr dup . 1- ?dup 0= until cr ." Launch!" cr ;

              Give a man a rocket and he will fly for a day; teach him to build and he will spend the rest of his days sanding...

              Comment

              • sandman
                Custom Cone, Kit & Decal Maker
                • Mar 2005
                • 5082
                • Way North of Detroit

                #8
                Originally posted by Bill
                Do both sides of the fin in one sitting instead of do one side, let it dry, then do the other side.


                Bill
                Oh, that's a given.
                "I'm a sandman. I've never killed anyone. I terminate runners when their time is up." Logan from "Logan's Run"

                http://sandmandecals.com/

                Comment

                • foamy
                  Master Modeler
                  • Jan 2011
                  • 1115
                  • The Land of Pleasant Living

                  #9
                  I'm with the Elmer's Fill 'n Finish. It covers a multitude of sins and I don't like wood grain showing.

                  I do my fins with it, sand them and then hit them with three coats of Deft. If they're warped, I flatten them between wax paper and heavy books for a few days. I then attach them and prime the rocket. If there's still grain showing it gets hit with Squadron Green, sanded and I can move right to the white coat.

                  Balsa nose cones get Fill 'n Finish, sanding, and then a soaked-in coat of CA and another sanding. Hardens them up nicely. Sometimes (depending on fin shape), I'll hit the edges of the fins with CA.

                  If the fins are long and thin (prone to breakage), I'll paper them. Papering is serious insurance.
                  Retro-grouch

                  Comment

                  • astronwolf
                    Lost his Drifter
                    • Mar 2013
                    • 1796
                    • Northeast Ohio

                    #10
                    I finish my fins before gluing them to the airframe, so I do see warps. But after treating both sides of the fin, the warp almost always goes away after the fill 'n finish dries. If not, I just flatten them under a heavy weight overnight. No problems.

                    I'll second the recommendation for laminating fins with paper. This adds a lot of strength, and makes the fins nice and smooth. I recently did this with ordinary paper and Scotch brand Quick Dry Adhesive (for paper). This is a fast method for fins. Doesn't work very well for nose cones.
                    -Wolfram v. Kiparski
                    NAR 28643 - TRA 15520
                    MTMA Section #606 President

                    Comment

                    • jetlag
                      Old BAR
                      • Aug 2006
                      • 2294

                      #11
                      I often will just wick super-thin CA into the nose cone and/or fins and let dry without using an accelerant. This way, I get a hardened surface less prone to dings, and the wood seals up nicely.
                      Sand a little when dry and use your favorite filler and proceed to finish as you like.

                      Papering, at least as I've done it as described by several, does not stand the test of time or the elements for me. You still have to seal the paper! For all the trouble, I think my way works best and adds a whole lot less weight and better strength. MUCH easier to fix, too, when a fin breaks if it's not papered.

                      As usual, YMMV!

                      Allen

                      Comment

                      Working...