    Clear Coat Hazing

    Anyone have any suggestions for clear coats. I tried the Krylon brand and it comes out either grainy or hazy. I am in Tennessee and we have major humidity! Any way to correct the hazing? Any/all help appreciated!
  • dvmanning
    Advanced Rocketeer SAM# 0455
    • Nov 2012
    • 112
    • Sparta, Missouri

    #2
    I have used the Krylon Acrylic Crystal Clear (Gloss) #851301 always with great results. I live in SW Missouri and have to deal with the high humidities. I choose to use the paints and clear coats on days of low humidity. Like you I have tried to use the Crystal Clear (Satin Clear) in the past and it has been on my avoid list for a long time. ( It, as you say hazed over as soon as it dried) I have never used it again. The cap should have given it away, the cap is clear but hazy. The key to a good finish with a clear coat is multiple light coats. Usually, I use the same clear coat as the Master Modeler or Testor's paint. The paint in the bottles is water based now, but the spray cans are still lacquer based requiring brush cleaner for clean up. Use of the Krylon Acrylic gloss clear coat is the exception, it has always given me a great finish.
    Each of us will have a different technique that can give us the finish that we want to achieve.
    David
    David Manning
    SAM # 0455

    Comment

    • ghrocketman
      President, MAYHEM AGITATORS, Inc.
      • Jul 2005
      • 15966
      • Nunya Bizznuss, Michigan

      #3
      Regular Testors or Testors Model Master are the only clearcoats I never have trouble with Hazing/Blushing in high humidity. This is due to their very 'tame' solvent package consisting of mainly Ethyl Acetate. It does not blush due to the relatively slow drying.
      Use of Krylon or Clear Dope blushes in high humidity.
      Butyrate Dope Clear in an airbrush can prevent this by mixing Brodak Retarder into the mix to slow drying.
      Forget Krylon.
      When in doubt, WHACK the GAS and DITCH the brake !!!

      Yes, there is such a thing as NORMAL
      , if you have to ask what is "NORMAL" , you probably aren't !

      Failure may not be an OPTION, but it is ALWAYS a POSSIBILITY.
      ALL systems are GO for MAYHEM, AGITATION, CHAOS, TURMOIL, FIASCOS, AGGRAVATION, INSTIGATION, NUISANCE-ACTION, and HAVOC !

      Comment

      • jeffyjeep
        Old Submariner
        • Jan 2009
        • 8465
        • Home of Wayne & Garth

        #4
        I don't use Krylon ANYTHING anymore. I use only Testors Dullcoat for flat coating and Acrylic floor polish for gloss coating. I sometimes have trouble with hazing when using the Testors when: 1) there's high humidity, or 2) I'm clearcoating outside and it's windy and the almost dry dullcoat oversprays the target.

        If it's humid and/or windy I spray the Dullcoat indoors--after I've sent "The Vixen" on an errand. She doesn't like the smell of it--and personally I don't either. I think it smells like fruity diarrhea....

        .....or.....

        .......something.
        Never trust an atom. They make up everything.

        4 out of 3 people struggle with math.

        Chemically, alcohol IS a solution.

        NAR# 94042
        SAM# 0078

        Comment

        • dvmanning
          Advanced Rocketeer SAM# 0455
          • Nov 2012
          • 112
          • Sparta, Missouri

          #5
          Reading the label on a Krylon Spray can indicates that for ideal results use in humidity conditions of no more than 85 %.
          David Manning
          SAM # 0455

          Comment

          • Doug Sams
            In Memoriam
            • Mar 2005
            • 3965
            • Plano, TX resident since 1998.

            #6
            Originally posted by dvmanning
            Reading the label on a Krylon Spray can indicates that for ideal results use in humidity conditions of no more than 85 %.
            I'm surprised there was a number on the can. I don't recall ever seeing a humidity number - usually just a max temperature.

            The key is really the dew point, which is a function of temperature and relative humidity. But that's probably too technical for them to put it on the label.

            All that said, I'm pretty danged sure that the old Krylon - the fast drying stuff - would blush at well below 85%RH in the Texas heat. I have too many dull looking paint jobs as proof

            BTW, not just Krylon, but any hot solvent paints - ie, any fast drying paints - are prone to blushing. That includes RustOleum's Painter's Touch line as well as most lacquers.

            FWIW, the "hot" solvents evaporate quickly, and when they evaporate, they absorb heat - they cool the air around them. In turn, the rapidly cooling moisture in the air condenses onto the finish - tiny droplets of water cause the paint to be dull.

            And that's also why huffing paint causes some people to be dull

            Doug

            .
            YORF member #11

            Comment

            • ghrocketman
              President, MAYHEM AGITATORS, Inc.
              • Jul 2005
              • 15966
              • Nunya Bizznuss, Michigan

              #7
              Agree here; Old formula Krylon and any Butryate Dope (without retarder in the mix) will definitely blush at 85% humidity....I don't like to spray dopw when humidity is over 70%; dark colors are virtually guaranteed to blush.
              When in doubt, WHACK the GAS and DITCH the brake !!!

              Yes, there is such a thing as NORMAL
              , if you have to ask what is "NORMAL" , you probably aren't !

              Failure may not be an OPTION, but it is ALWAYS a POSSIBILITY.
              ALL systems are GO for MAYHEM, AGITATION, CHAOS, TURMOIL, FIASCOS, AGGRAVATION, INSTIGATION, NUISANCE-ACTION, and HAVOC !

              Comment

              Working...