    I don't remember which of Rokitflite's Deuces/Pharoah's Wild threads it was (either here or over at TRF) in which Scott mentioned doing three layers of yellow glue fillets followed up by a final epoxy fillet.

    Is this the norm? Admittedly, the Pharoah's Wild is a beautiful example of rocket building/finishing craftsmanship but I'm wondering if I really need to go to those lengths for a bird I'm just going to fly at the park until I lose it. I'm all about the flying and thought I was going overkill when I used JAL3's method of poking pinholes under and beside the fins for the glue and fillets to penetrate. BTW, that seems to have worked pretty well.

    Anyway, before I start to ramble (too late!), what's everyone think about this?
    Kit (aka Cranky Kong)

    I'm just a roadie for the banned...
  • Intruder
    Craftsman
    • Oct 2007
    • 278
    • Huntingdon, Tennessee

    #2
    Unless your ghrocketman, yes it's overkill. One layer of glue is plenty for LPR and the lower end of MPR rockets.

    Comment

    • snaquin
      The_Ripper
      • Jun 2005
      • 1948
      • Louisiana

      #3
      Everyone will have an opinion about glue and fillets ..... and there's plenty of adhesives and fillers to choose from!

      Bearing that in mind, if you're going to finish up with an epoxy top coat for the final fillet I'd use CA to get a quick fin attachment and then one epoxy fillet. Epoxy fillets can be applied in one application.

      Use blue painters tape on the airframe and on the fin to keep the epoxy from flowing where you don't want it. Some guys use a little tape to dam up the front and rear part of the fin so the epoxy don't flow over the edge but I find 5-min Devcon sets up so fast it's not a problem. Immediately after the fillet is applied smooth it once with a craft stick and remove the blue tape before the epoxy sets completely.

      Majority of my builds are mid power and I get a nice fillet in one application. I get all three fins done in a short time ..... mounted and fillets. I doubt you'd find many using this method with model rockets. If the fillets are small it doesn't add much weight.



      .
      Attached Files
      Steve Naquin
      TRA# 677 L2
      NAR# 85518
      SAM# 0052

      In Construction: TBD
      In Paint & Detail: TBD
      In Build Queue: TBD
      In Repair: TBD
      2025 Fall Launch Dates: Sept. 27-28 (Rain Date Oct. 4-5), Nov. 1-2 (Rain Date Nov. 8-9)

      Comment

      • Bazookadale
        I wish I was a spaceman!
        • Jan 2006
        • 431
        • Elizabethtown,PA

        #4
        Originally posted by o1d_dude
        I don't remember which of Rokitflite's Deuces/Pharoah's Wild threads it was (either here or over at TRF) in which Scott mentioned doing three layers of yellow glue fillets followed up by a final epoxy fillet.
        I've never heard of that - IMHO if you mix adhesive types like that you should wait a coupla days to be sure the yellow glue has completely cured, because I can't see it curing well with epoxy over top.
        Just my opinion
        Did the chicken really cross the road, or did the
        road move beneath the chicken? Albert Einstein

        You Can't break the laws of physics but they can break you. Christine McKinley


        Dale Greene

        Mentor, Penn Manor Rocket Club

        VISIT SPAAR
        2010 Calder Cup
        The Old West
        2009 Calder Cup

        " Speaking the Truth in times of universal deceit is a revolutionary act. " George Orwell

        Comment

        • Mark II
          Forest Sprite
          • Dec 2006
          • 3657
          • Back Up in the Woods

          #5
          For LPR, the carpenter's glue alone should be sufficient. I would put down a couple of layers; three layers would be the outside limit, and that would only be for larger LPR models. I use gap-filling (or medium cure) CA to bond my fins to the airframe, and then fillet with something that can be spread and smoothed down. You don't hear about too many people using CA for fin bonding, but I have never had any of my models lose any fins that were bonded with a quality medium-cure CA.

          For my largest LPR models (think Super Big Bertha or Maxi Alpha) and up into the mid-power stuff that I'm doing now, I use epoxy for filleting over the CA. Bob and Steve are right - you only need one application of it. But I prefer slow-cure or 30 minute epoxy. The long cure gives it plenty of time to level, and it gives me plenty of time to smooth it down to a small but strong fillet. (The slow-cure formulation produces a stronger bond and a harder fillet than the faster varieties.) Also, the tip about masking off the fin and body tube areas around the fillet is a great one - my fin fillets look SO MUCH BETTER since I started doing that. But you do have to check on it periodically for the first half-hour or so, and you need to keep the fin root level and undisturbed for a few hours. Because of that, you can only do a single fillet at a time when you use the slow cure. For masking off the fillets, I use Duck brand "Easy Release," or lightest tack, masking tape (the purple stuff). I get it at Walmart. I remove it as soon as I can, once everything looks like it has stabilized. (Another good reason to use slow-cure - it gives you more leeway over when you will need to remove the masking tape. But definitely take it off before any real curing occurs, or it will be permanent.)

          Not everyone creates little "dams" at the top and bottom of the fin root when they apply epoxy for fillets, and I don't either. When I did that in the past, I wound up with blobs of built-up epoxy at both ends of the root. Now I use a lighter hand when I apply the epoxy, and I keep the fillets small. I don't have the same problems with overflowing and run-off that I used to get before I started doing that. (And the masking really helps, too.) I put on a nitrile glove (latex is not epoxy-proof) and "smooth" the fillet down with a finger that has been lightly dampened with denatured alcohol or acetone. But I don't really do it to smooth the fillet; the epoxy levels itself, so I don't have to do that. I do it instead to wipe off any excess, so that I can get the fillet down to a nice thin layer.

          I have had problems with fast 5 minute epoxy curing too fast, leaving me with thick, chunky fillets that were tough to sand down. But do try different adhesives and methods and decide what works best for you.

          I agree with Dale's point as well. If you apply a second type of adhesive on top of one that has not fully cured, neither adhesive will bond well or be very strong. I usually wait at least a day for even my CA to cure before I start applying fillets. After all, what's the rush?

          BTW, applying "glue rivets" is one of those classic pieces of advice that is almost as old as the hobby itself. It is a GREAT technique that has stood the test of time. I would not be shy about using it.

          MarkII
          Last edited by Mark II; 03-13-2009, 09:37 PM.
          Mark S. Kulka NAR #86134 L1,_ASTRE #471_Adirondack Mountains, NY
          Opinions Unfettered by Logic • Advice Unsullied by Erudition • Rocketry Without Pity
          +09281962-TAK-08272007+
          SAM # 0011

          Comment

          • mycrofte
            Trust me, it'll work!
            • Mar 2009
            • 1930
            • Illinois

            #6
            They all sound good, depending on what you want. I put my fins on with super glue gel, then 5-Minute epoxy the fillets. Except I don't take the precautions. I just run my pinkie down it to get out the excess epoxy. Makes a nice concave fillet without the tape.

            I tried using the wood glue in the fillet but it dries lumpy. Thereby, taking 3 layers to smooth it out. I did have one lumpy epoxy fillet when the 5-Minute started to cure on me. So you have to work fast or mix smaller amounts.

            Comment

            • Bob Kaplow
              Mr. Dual Eggloft
              • Aug 2008
              • 585
              • Illinois: where our Governors make our license plates.

              #7
              Originally posted by mycrofte
              They all sound good, depending on what you want. I put my fins on with super glue gel, then 5-Minute epoxy the fillets. Except I don't take the precautions. I just run my pinkie down it to get out the excess epoxy. Makes a nice concave fillet without the tape.

              I tried using the wood glue in the fillet but it dries lumpy. Thereby, taking 3 layers to smooth it out. I did have one lumpy epoxy fillet when the 5-Minute started to cure on me. So you have to work fast or mix smaller amounts.
              I would NEVER use 5 minute epoxy for fillets, or for any thing else! Peanut butter would add just about as much strength, especially to a minimum diameter model or TTW design subject to motor heating.

              For fillets get the slowest cure epoxy you can get, and let time work for you to level it out and give you glass like fillets. The only epoxies I use any more are the slow cure laminating resins. When I need something added to them, I pick the filler and add it myself

              If you haven't tried the System Three trial kit, do yourself a favor and get one now. You'll never go back. It's got enough stuff for years of MR construction, or several Level 1 sized rockets.
              I fought the law, and the law LOST!

              Comment

              • mycrofte
                Trust me, it'll work!
                • Mar 2009
                • 1930
                • Illinois

                #8
                Never heard of it. I'll have to give it a try!

                Thanx

                Comment

                • Solomoriah
                  Incorrigible Kit Basher
                  • Jul 2006
                  • 1940
                  • USA

                  #9
                  I put epoxy fillets on my biggest rockets only, using the 50 minute DevCon (I think that's the brand) which I get at Wal-Mart. When I'm going to use epoxy fillets, I attach the fins using yellow glue and give them a day to dry before applying the epoxy.

                  Yellow glue works fine for smaller models, though.
                  NAR # 115523
                  Once upon a better day... SAM #0076
                  My site: http://rocketry.gonnerman.org

                  Comment

                  • snaquin
                    The_Ripper
                    • Jun 2005
                    • 1948
                    • Louisiana

                    #10
                    Not all 5-minute epoxies are created equal .....

                    DevCon 5-minute is actually one of the better store brands you can buy for the price and I get it at Wal-Mart too. DevCon 30-minute is stronger and allows more working time. I've tried several brands over the years and DevCon and AeroPoxy in the quick cures are the two I like the best.

                    They are self-leveling whereas other 5-minute brands are not so forgiving. I find the working time for the 5-minute sufficient and they are very strong. I mix it well in a small disposable bathroom cut for about a minute, apply it between the tape masking and swipe with a craft stick. It generally only takes two to three minutes and I'm pulling the tape. Website & specs for the two brands I use most often are here:

                    http://www.devcon.com/products/produ...m?familyid=175

                    http://www.devcon.com/prodfiles/pdfs/fam_tds_175.pdf

                    http://www.ptm-w.com/index.asp?pgid=177

                    http://www.ptm-w.com/showDoc.asp?fna...20bulletin.pdf

                    .
                    Steve Naquin
                    TRA# 677 L2
                    NAR# 85518
                    SAM# 0052

                    In Construction: TBD
                    In Paint & Detail: TBD
                    In Build Queue: TBD
                    In Repair: TBD
                    2025 Fall Launch Dates: Sept. 27-28 (Rain Date Oct. 4-5), Nov. 1-2 (Rain Date Nov. 8-9)

                    Comment

                    • snaquin
                      The_Ripper
                      • Jun 2005
                      • 1948
                      • Louisiana

                      #11
                      Originally posted by mycrofte
                      Except I don't take the precautions. I just run my pinkie down it to get out the excess epoxy..
                      Sounds like you are aware of the precautions but take my advice and don't do this. You will eventually develop an allergic reaction by direct contact with the skin with this stuff it's just a matter of time. I did this for years exactly like you describe and now I have allergic reactions to epoxy. I always use gloves now .....

                      .
                      Steve Naquin
                      TRA# 677 L2
                      NAR# 85518
                      SAM# 0052

                      In Construction: TBD
                      In Paint & Detail: TBD
                      In Build Queue: TBD
                      In Repair: TBD
                      2025 Fall Launch Dates: Sept. 27-28 (Rain Date Oct. 4-5), Nov. 1-2 (Rain Date Nov. 8-9)

                      Comment

                      • rokitflite
                        Master Modeler
                        • Mar 2005
                        • 952

                        #12
                        It was 2 fillets of carpenters glue and a final, thin fillet of 15 minute epoxy... Not for additional strength, but for a smooth, bubble free fillet. And uh, yeah, I am aware that the yellow glue needs to dry before putting epoxy over it.