    Papering.

    This is a new technique to me. I had never heard of it until about a week ago. I was taught the old school way of dealing with fins wood filler, sanding, sanding sealer, primer, paint. Aparently you can save alot of money by laminating the fins in paper. I saw this done on Rocketreviews.com. It seems to me though it would strenthen the fin but weeken its attachment, even if it wasnt papered at the root. Wouldnt it make the fillets week? It looks like most people are using self adhesive label paper to do this.
    Being interested in this new to me technique I have decided to try it out on a an unusable fin I have. Insted of using self adhesive paper though I am using regular white paper with a thin layer of elmers all purpose glue. Once the glue dries im going to paint it and see the outcome verses my tried and true old school method. That being said though, those of you who have experience in papering could you give some of us who dont know much about it some pointers?
  • gpoehlein
    Paper Rocketeer
    • Mar 2005
    • 1181
    • Evansville, Indiana

    #2
    Be careful with the glue and regular paper - too much glue and you stand a chance of warping the balsa. It will help if you laminate both sides at the same time and press under a weight (assuming you are laminating it before attaching to a rocket). When I've done this with label stock, I've applied the label stock to the fin after it was attached and filleted (Super Alpha).

    I've also used this to strengthen fins that have been damaged and repaired - you can cut the label stock to fit and have about a half inch tab at the root, with creates a very strong "fillet".

    A third technique that makes for an incredibly tough fin is to coat the fin in CA and place the paper on it. Soak a little more CA into the paper, sandwich between two pieces of wax paper and press under a weight. When it dries, you can sand it smooth as glass and it will be tough as plastic.

    Greg
    Greg Poehlein

    Member of Launch Crue - http://launchcrue.org/

    Hint #1: Do not use magician's flash paper for recovery wadding!

    Hint #2: Clean your shoes after flyin' in that cow pasture - that ain't no dirt clod on the sole!

    Comment

    • STRMan
      Master Modeler
      • Nov 2007
      • 873
      • USA

      #3
      I haven't had much luck getting a super smooth surface using Elmer's glue to laminate paper onto fins. I like using the self adhesive paper method. Once the fins are laminated, I then coat the edges with CA. I like the purple Crazy Glue version with the brush in the cap. I seal all the edges except for the root of the fin. It goes on purple and cures clear.

      I then gently sand these edges down smoothly. This technique works great on fins with squared off edges.

      I then glue and fillet the fin in place as usual. I have never had even one rocket done this way delaminate or fail in any manner.

      When priming, go slowly, very slowly. Make sure the first few coats of primer on the paper is very, very light, almost a dusting. If you put on a thick first coat, the paper will soak it up and get wrinkled. Don't ask me how I know this.

      After a good primer treatment, top coats can by put on in the usual manner.
      "AND I hope they are from the planet of the "Chunk spunky Mary-Lou Retton clones". - Ironnerd

      "Those who trade liberty for security have neither" - Benjamin Franklin

      "Semroc is almost always the answer" - Stefanj

      www.paulsavia.com

      www.soundclick.com/paulsavia

      Comment

      • metlfreak
        Craftsman
        • Sep 2009
        • 114

        #4
        Originally posted by STRMan
        I haven't had much luck getting a super smooth surface using Elmer's glue to laminate paper onto fins. I like using the self adhesive paper method. Once the fins are laminated, I then coat the edges with CA. I like the purple Crazy Glue version with the brush in the cap. I seal all the edges except for the root of the fin. It goes on purple and cures clear.

        I then gently sand these edges down smoothly. This technique works great on fins with squared off edges.

        I then glue and fillet the fin in place as usual. I have never had even one rocket done this way delaminate or fail in any manner.

        When priming, go slowly, very slowly. Make sure the first few coats of primer on the paper is very, very light, almost a dusting. If you put on a thick first coat, the paper will soak it up and get wrinkled. Don't ask me how I know this.

        After a good primer treatment, top coats can by put on in the usual manner.
        Awsome. The elmers glue has to be put on smoothed thin. Label paper with a fillet to secure it good might be the "safest routs to go when papering. No chance of warping and gives you more controle.
        **Thanks for the priming advice. I was thinking it might wrinkle.

        Comment

        • metlfreak
          Craftsman
          • Sep 2009
          • 114

          #5
          Originally posted by gpoehlein
          Be careful with the glue and regular paper - too much glue and you stand a chance of warping the balsa. It will help if you laminate both sides at the same time and press under a weight (assuming you are laminating it before attaching to a rocket). When I've done this with label stock, I've applied the label stock to the fin after it was attached and filleted (Super Alpha).

          I've also used this to strengthen fins that have been damaged and repaired - you can cut the label stock to fit and have about a half inch tab at the root, with creates a very strong "fillet".

          A third technique that makes for an incredibly tough fin is to coat the fin in CA and place the paper on it. Soak a little more CA into the paper, sandwich between two pieces of wax paper and press under a weight. When it dries, you can sand it smooth as glass and it will be tough as plastic.

          Greg
          The one I did last night with the elmers glue and regular paper came out very nice. It didnt warp and the glue, even though it was smeard on thin dried pretty hard. I havent painted it yet, but I will shortly to see how it comes out.

          As far as wrinkling I think the glued aproach will keep the paper from doing so. However I like the idea of self adhesive because its quiker, but it wont harden like the glued method does.

          Comment

          • rocketguy101
            frustrated aero
            • Sep 2006
            • 900
            • Duncan, OK

            #6
            If you are worried about fillets after papering, try "glue rivets" shown below. I use the holes in the fin root and tube on all my rockets. Double gluing the fin root really strengthens the joint too (apply thin layer of glue to both surfaces, allow to dry, then apply glue and press the parts together)
            Attached Files
            David Stribling

            Comment

            • mycrofte
              Trust me, it'll work!
              • Mar 2009
              • 1930
              • Illinois

              #7
              What worked best for me was to get the fins coated and sanded once to be semi flat. Then cut one paper to fit and the other side over sized. I found making both sheets over sized makes it hard to tell where to cut at first.

              Then I apply Elmer's to one side and squeegee half of it off to apply the cut piece. Then flip it over and do the other side. Laying it on an over sized piece so my aim doesn't have to be perfect. Then it all goes between wax paper and under a pile of hardback book for 48 hours.

              After that is done, then I sand the round edges. I end up with fuzzy edges that need glued and re-sanded. But works best for me. I tried papering after sanding but ended up with loose edges that took twice as much work to fix.

              Comment

              • CPMcGraw
                In Memoriam
                • Mar 2005
                • 5357
                • Mobile, Alabama

                #8
                While I regularly use the self-stick label paper, I have also used plain paper with 3M's spray adhesives. They have two formulas that work great -- 77 and 90. Formula 77 is a general-purpose contact adhesive with a 'medium hold', while formula 90 is a 'strong' hold. The 90 is great for attaching embossed paper wraps around large Saturn models...

                It is a little messy, compared to the self-stick paper, but the holding power is much better.

                One thing to remember, no matter which method you choose, is to keep the root edge free of any glue until the time you are attaching it to the tube. When applying the CA to the paper edges, stay away from the root edge. The CA is only meant to harden the wood around the outer perimeter for a smooth round-over, and to seal the paper so it doesn't delaminate from the wood.

                A sideline method using white glue: Apply a thin layer to both sides of the fin and the paper, then let them dry completely. Take a Monokote iron and heat-press the paper onto the fin. What this will do is liquefy the glue briefly, allowing for a very smooth surface, then it hardens just as quickly when the iron is removed. With this method, it might be possibly to skip the CA step. YMMV.
                Craig McGraw

                BARCLONE Rocketry -- http://barclone.rocketshoppe.com
                BARCLONE Blogsite -- http://barclone.wordpress.com
                BARCLONE Forum -- BARCLONE Forum

                BARs helping BARs

                SAM 0044
                AMA 352635

                Comment

                • blackshire
                  In Memoriam
                  • Jan 2009
                  • 6507
                  • Fairbanks, Alaska

                  #9
                  I've achieved excellent results simply by spreading a very thin film of yellow wood glue or white glue on one side of a fin using a finger, then pressing the glued side down onto a sheet of typing paper or copier paper. After a couple of minutes, I flip the sheet of paper over on a smooth surface, lay another sheet of paper over it, and gently rub all along where the fin is underneath to smooth out any bulges of glue.

                  When the glue is dry, I cut the fin out of the sheet of paper and repeat the process on the other side of the fin. The finished fins are perfectly smooth, and before sanding their edges I seal them with glue. After gluing the fins onto the body tube (always using G. Harry Stine's double-glue joint method) and letting them dry, I apply glue fillets, which adhere as well to the paper as they do to un-papered balsa fins.
                  Last edited by blackshire; 10-11-2009, 11:55 AM. Reason: This ol' hoss done forgot somethin'.
                  Black Shire--Draft horse in human form, model rocketeer, occasional mystic, and writer, see:
                  http://www.lulu.com/content/paperbac...n-form/8075185
                  http://www.lulu.com/product/cd/what-...f-2%29/6122050
                  http://www.lulu.com/product/cd/what-...f-2%29/6126511
                  All of my book proceeds go to the Northcote Heavy Horse Centre www.northcotehorses.com.
                  NAR #54895 SR

                  Comment

                  • metlfreak
                    Craftsman
                    • Sep 2009
                    • 114

                    #10
                    I just brush painted the experiment fin I did. It has got to be very thin coats because even being careful it tried to wrinkle on me a little. The next fin im going to prime then paint. To see the over all affect then compare.

                    Comment

                    • blackshire
                      In Memoriam
                      • Jan 2009
                      • 6507
                      • Fairbanks, Alaska

                      #11
                      Originally posted by metlfreak
                      I just brush painted the experiment fin I did. It has got to be very thin coats because even being careful it tried to wrinkle on me a little. The next fin im going to prime then paint. To see the over all affect then compare.
                      Yes, an excessive amount of yellow wood glue or white glue can cause wrinkling of the paper. Fortunately, you only need to use a very small amount of glue to achieve a "printed circuit board-hard" finish with the paper/glue composite. For smaller fins, I just rub on enough glue with a fingertip to barely coat the wood. With larger fins (bigger than those on the Estes Alpha or Quest Astra), I often use a piece of scrap sheet balsa with a straight edge as a "squeegee" to rub a uniformly thin layer of glue onto the fins.
                      Black Shire--Draft horse in human form, model rocketeer, occasional mystic, and writer, see:
                      http://www.lulu.com/content/paperbac...n-form/8075185
                      http://www.lulu.com/product/cd/what-...f-2%29/6122050
                      http://www.lulu.com/product/cd/what-...f-2%29/6126511
                      All of my book proceeds go to the Northcote Heavy Horse Centre www.northcotehorses.com.
                      NAR #54895 SR

                      Comment

                      • Doug Sams
                        In Memoriam
                        • Mar 2005
                        • 3965
                        • Plano, TX resident since 1998.

                        #12
                        Originally posted by metlfreak
                        The next fin im going to prime then paint.
                        Yes, you need to do this. The key benefit of papering (besides stiffening the fin) is to make finishing easier by eliminating most of the filling (of the grain). But you still need to prime and sand prior to applying a finish coat. Maybe prime twice. If you just put the paint on the paper...well, it's not gonna turn out very pretty.

                        Doug

                        .
                        YORF member #11

                        Comment

                        • metlfreak
                          Craftsman
                          • Sep 2009
                          • 114

                          #13
                          Originally posted by Doug Sams
                          Yes, you need to do this. The key benefit of papering (besides stiffening the fin) is to make finishing easier by eliminating most of the filling (of the grain). But you still need to prime and sand prior to applying a finish coat. Maybe prime twice. If you just put the paint on the paper...well, it's not gonna turn out very pretty.

                          Doug

                          .
                          Agreed. It looked.....well smooth but rough if that makes since.

                          Comment

                          • Intruder
                            Craftsman
                            • Oct 2007
                            • 278
                            • Huntingdon, Tennessee

                            #14
                            If you want to round or taper your fins, be sure to do that before you paper them. Sanding all that glue soaked paper and balsa will NOT be a pleasant experience (trust me).

                            Comment

                            • mycrofte
                              Trust me, it'll work!
                              • Mar 2009
                              • 1930
                              • Illinois

                              #15
                              Yeah, I sand after, and it takes a while to get all the fuzz out. It just works better for me...

                              Comment

                              Working...