    Priming And Painting

    I've filled the balsa grain on the fins. I've covered the spirals with three coasts of the current brand of the old Elmer's Fill & Finish. Now, I'd like to paint the model with sandable primer. I have some questions:

    I see that Krylon has at least four different colors of sandable primer. 1)Does the final paint scheme of the model determine the best color of sandable primer to use? 2). What's the best painting technique for applying the primer, 1.e. number and thickness of coats, grade of sandpaper to use, and just exactly what areas of the model should be coated, and how much primer should be sanded off when it dries?

    Once the model is properly primed, should there be an undercoat applied before the final coat of paint is sprayed? If so, what color undercoats match up the best with top coats?
    A person will seldom remember your exact words to him or her ,but they won't forget how you made them feel
  • ScaleNut
    Craftsman
    • Apr 2005
    • 269
    • Heart of the South

    #2
    I don't see sandable primer on the website.
    They used to have a really good sandable primer several years ago, than the switch to a thin more paint like primer. If they brought that back it would be good news !

    As far as primer color I normally use what ever color I have on hand than give the rocket a spray of white paint. This works great for all colors, Except in the case of silvers,golds,coppers..ect. those colors seem to work best over black.

    Comment

    • stefanj
      Master Modeler
      • Mar 2005
      • 3086
      • Hillsboro, OR

      #3
      Put on coats one at a time. Let dry THOROUGHLY. Dryer primer means easier sanding.

      The first coat or so should be sanded almost entirely off; you're filling in scratches. Use 400 grit and/or 600 grit.

      Later coats should actually coat. Wet sand, pausing to wipe down the model now and then. Inspect before the next coat; fill in remaining dings with brushed-on gray enamel. After the enamel is dry sand it smooth.

      The final sanded coat should end up glossy and smooth, no trace of grain or gaps or seams.

      Don't go crazy trying to get a perfectly smooth and glossy final paint coat. Make it a little heavier than the initial coats. Let dry THOROUGHLY, then use automotive polishing compound ($2.00 a tub!) to get the gloss you're looking for.

      Then, clear coat, decals, and a final clear coat.
      NAR #27085 - Oregon Rocketry - SAM

      Comment

      • o1d_dude
        Certified Rocket Monkey
        • Dec 2008
        • 551
        • The failed Socialist State of California

        #4
        Rustoleum makes a good sandable primer that goes on thick and sands nicely when it's dry. I use nothing else.

        StefanJ nailed it. I'm a little more obsessive/compulsive about sanding and start with 220, then 320, 400, and finish up with 600 grit. You can get a finish like glass if you want to put in the time and effort.

        If you're eager to fly, build an Estes Blue Ninja or one of their other basic rockets. Fly those as needed and it will keep you working on your "good" rockets until they're done. =)
        Kit (aka Cranky Kong)

        I'm just a roadie for the banned...

        Comment

        • AFlyingMonkey
          young man but an old hand
          • Oct 2009
          • 121
          • Overland Park, Kansas

          #5
          I use Rustolium Painter's Choice that can be found at Home Depot. wet sand-able and has a ton of talc in it. works really really well. i've seen people use this for filling in grain and spirals without doing anything else. now of course the rocket is heavier but it works.
          She said, "Don't make me release the flying monkeys!"

          Too late, I'm here......

          Comment

          • zog139
            Rocketry is Fun.... Darn It !
            • Mar 2007
            • 220
            • Maryland

            #6
            I dont use Krylon primer at all anymore. I find that it gums up sandpaper and is all around difficult to use.

            Look for high build or spot fill primer. Sometimes the automotive brands have these types available.

            My favorite primer to use currently is the Plastikote brand Spot Fill and Primer
            Jim Filler
            NARHAMS # 139
            NAR CB - RCPC

            Comment

            • Marlin523
              Marlin523
              • Jun 2008
              • 9
              • Fishers, IN

              #7
              I also use Rustoleum Sandable Primer. Dries quickly and sands very well. I've used all kinds of enamels over this and have had no problems. The idea of almost sanding off the first coat is a good one if you want a really great finish. Of course, you must re-apply the primer coat and sand again. I've done this as many as three ooats for a great finish. The primer will show you your "problem" areas.

              Comment

              • luke strawwalker
                BAR
                • Dec 2007
                • 6151
                • Needville and Shiner, TX

                #8
                Good advice all around...

                I use the Walmart Colorplace 99 cent a can primer and I've had good luck with it. They make a red primer that's got more solids in it (fills a bit better-- kinda like Hi-build primer) and the regular gray primer, which I use most of the time. It goes on smooth and dries fast. I usually give about 2-3 light coats and then sand, starting with 220 grit to take most of it off, then switching to 600 grit wet/dry and dipping the paper in water to prevent clogging-- as you sand the moisture will mix with the sanded off paint residue and form "sanding mud" that you periodically wipe off with a paper towel. I inspect the rocket against a light "gleaming" off the tube as I turn it slowly looking for imperfections, and sand it down more if needed. If I see anything obviously wrong (sanded completely through the primer in spots, etc.) I reprimer it before switching to the 600 grit.

                I only use those two paper grits and if you do it right you can make a rocket like a mirror without too terribly much effort... sand in small circles keeping the rocket and paper moving AT ALL TIMES; don't stop and sand continuously on one spot or you'll get flat spots, sand-thrus, etc. that will make an ugly finish. Let the paper do the work-- don't push hard or try to take too much off at one time. The 200 grit leaves SOME sanding scratches behind, but the 600 wet/dry and water will take them out if you do it right and leave the tube slick and smooth and shiny when you're done.

                Good luck! OL JR
                The X-87B Cruise Basselope-- THE Ultimate Weapon in the arsenal of Homeland Security and only $52 million per round!

                Comment

                • Pem Tech
                  Retromaniac
                  • Oct 2008
                  • 298

                  #9
                  Originally posted by AFlyingMonkey
                  I use Rustolium Painter's Choice that can be found at Home Depot. wet sand-able and has a ton of talc in it. works really really well. i've seen people use this for filling in grain and spirals without doing anything else. now of course the rocket is heavier but it works.

                  Yep, this is what I use as well and it will fill balsa and spirals without a filler.
                  Layne Pemberton NAR# 83083
                  Mad Scientist, Minion and Owner
                  PembertonTechnologies.com
                  P.O. Box 250760
                  North Little Rock AR, 72225

                  L1 on Pem-Tech Space Ark
                  at NSL2007

                  pem_tech (at) Yahoo (dot) com
                  TRF (at) pembertontechnologies (dot) com

                  Comment

                  • jharding58
                    Master Modeler
                    • Apr 2007
                    • 1936
                    • Kennesaw, GA

                    #10
                    I have finally succumbed to the delights of Plasti Kote sandable primer (#466). I have read about it, thought about it, and with a return to building decided to try it. Three spray coats with a light wet sand on the last coat and two colour coats gave me this. I think I like it.
                    Attached Files
                    Gravity is a harsh mistress
                    SAM 002
                    NAR 91005
                    "The complexity of living is eminently favored to the simplicity of not."

                    Comment

                    • dvmanning
                      Advanced Rocketeer SAM# 0455
                      • Nov 2012
                      • 112
                      • Sparta, Missouri

                      #11
                      Priming and Painting

                      For those of you that will think , I take a long time to put the finish on a model rocket, I agree I do, but the results speak for themselves. Having the hobby of woodworking, starting in seventh grade and continuing on into my retirement years. I have developed the habit of not getting in a hurry when I put a finish on it.

                      I start by sanding all my balsa parts with 320, then 400 and then 600 or 800 wet/dry automotive sandpaper. If the parts are small, I usually glue them to the tubes first and sand them later. The larger parts, fins , etc. I sand while they are still in the sheet

                      I shape all of my edges whether they are the leading edge, trailing edge, outside edge or the root edge. I always sand the root edge to conform to the curve of the tube for better contact with the tube. It is important to lightly sand all of the tube stock to take of the waxy surface an the shine for better contact.

                      I prefer the Aerosol Sanding Sealer in Spray Cans sold by Lowes. I lightly spray the first coat, let it dry overnight, apply the second coat, let it dry overnight and then sand using the grits mentioned above. The final coat is used only on areas that need it.

                      I use either the Tester's primer or Master Modeler Primer. White for light colored paint and gray for darker colors. I normally do a light coat and then a heavier coat. Lightly sand between coats

                      Final colors have two coats , a light first coat and the final coat. I usually don't sand final coats. I then apply two coats of clear coats and let dry between coats Add my decals and them apply a model wax to the finished model. And yes, I let it dry before I buff it out.

                      The end result is a model that looks like it is made of aluminum instead of balsa.

                      I use model putty on occasion to take care spaces between parts or to help contour the part.
                      I use miniature file sets in 4 inches and 6 inches and stylus tools to shape areas when needed such as the glue fillets on fins and tube.
                      I let each coat dry overnight
                      David Manning
                      SAM # 0455

                      Comment

                      • wz2p7j
                        Craftsman
                        • Jun 2011
                        • 104

                        #12
                        I usually hit my rockets with 15-20 coats of primer to hide all the spiral winding marks and the general unevenness of most kit's BT's. I see some guys saying 3 coats primer but I'm not even sure how that's possible to hide the spiral lines, at least on the Estes or Semroc kits I usually build.

                        Chris

                        Comment

                        • dvmanning
                          Advanced Rocketeer SAM# 0455
                          • Nov 2012
                          • 112
                          • Sparta, Missouri

                          #13
                          Priming and Painting

                          Chris, that many coats of primer is not necessary. Get you a BT 50 tube about 10 inches long,
                          lightly sand the tube with a fine sandpaper to rough up the tube body. This is for test purposes. Now place tape on both sides of the spiral and cover the area between the spirals. With clear gloves on, spray a light coat sanding sealer over the spirals between the tape and set aside to dry. With the tape still on the tube lightly sand the spirals between the tape. Spray a second and heavier coat of the sanding sealer and let it dry. Again lightly sand the spirals and remove the tape. Now when you lightly spray the entire tube with the sanding sealer and let it dry and then lightly sand it, you should not be able to see the spirals. one light coat of primer and let dry. lightly sand. Now spray a good light coat of color and lightly sand. Then add the second and final color coat and let dry. Now spray a light clear coat and let dry overnight, Now for the final clear coat on the tube. It is at this time I would apply the decals and the a coat of model wax.
                          For those builders who are impatient or get in a hurry this method will not work . For those of us who have time to take the time to do things one step at a time the result will be flawless.
                          This not only will make the spirals disappear, but any imperfections will disappear as well.

                          When I build custom furniture, the finish will take me seven to ten days, to get a finish that will show depth as well as be able to see you face in it.
                          David Manning
                          SAM # 0455

                          Comment

                          • wz2p7j
                            Craftsman
                            • Jun 2011
                            • 104

                            #14
                            Well maybe it's not 15-20 coats. But it's not 3 either. I keep hitting it and sanding it until the spirals disappear and, I'm not sure what to call it, but the peaks and valleys disappear as well. Hit it with the air brush. Sand with 1000 grit, thin the paint a little more and hit it with the air brush again. Decal then clear with enamel if I feel lucky. Never use Future - effed up too many rockets.

                            Chris

                            Comment

                            • dvmanning
                              Advanced Rocketeer SAM# 0455
                              • Nov 2012
                              • 112
                              • Sparta, Missouri

                              #15
                              Chris, I don't use the Future stuff either, but, I just never thought that it would do the job. The model wax can be purchased at Hobby Lobby is small quantities in a set with a small amount of sanding sealer.
                              I use Deft Lacquer Sanding sealer in aerosol spray that I got at Lowe's. My last two cans I purchased at our local Ace Hardware and he ordered them for me. For what ever reason our local Lowe's just quite carrying it. I have also used a can of paste wax and it worked well. I don't use much on the rockets.
                              David Manning
                              SAM # 0455

                              Comment