* 'High build' primer with excellent adhesion for semi-rigid and flexible plastics
* All the same characteristics of SPOT FILLER with the addition of being flexible
Typically those primers loaded heavy with hot Aromatic solvents (Toluene, Xylene, Acetone, Ethyl Acetate, MEK, MIBK) capable of softening plastics if not careful are called "Lacquer based" and those with slow drying Aliphatic solvents that cannot be recoated anytime are called "Enamel" primers.
The higher the MgSi (Talc) content, the better they tend to fill.
Zinc Molybdate would give the primer a dark color (Is this a dark grey "hot rod black" primer ?).
Titanium Dioxide is straight white pigment that was first used years ago as a safe replacement for white lead.
Have no clue why Zinc Phosphate is in there.
As far as the percentages of the Aromatic Solvents, the higher the Acetone content and the lower the Toluene content the faster it will dry due to the evaporation points of the solvents.
Ethylbenzene (next slowest), Xylene, MEK and MIBK (next fastest) are all in between Toluene and Acetone as far as evaporarion rates.
When in doubt, WHACK the GAS and DITCH the brake !!!
Yes, there is such a thing as NORMAL, if you have to ask what is "NORMAL" , you probably aren't ! Failure may not be an OPTION, but it is ALWAYS a POSSIBILITY.
ALL systems are GO for MAYHEM, AGITATION, CHAOS, TURMOIL, FIASCOS, AGGRAVATION, INSTIGATION, NUISANCE-ACTION, and HAVOC !
Plastikote Spot Filler and Primer. Grey. The Red Oxide I have found tends to clog within the first use.
I've tried Duplicolor's product and it will do, better than any other, but Plastikote is the way to go.
My current finishing regimen:
Shoot one coat of SF&P.
lightly sand off the roughness.
Apply watered-down Elmer's Carpenters Wood Filler (or Fill'n'Finish if you've got some), to fill in the deepest valleys, dry, sand lightly.
Shoot successive coats of SF&P, sanding lightly between each one, until satisfied. Use a strong light and look along the surfaces toward the light to see remaining imperfections.
You *can* skip the wood filler step, and just use the SF&P. I just find it accellerates the process, and doing it AFTER the first coat of SF&P removes the threat of warping fins and such.
My favorite primer is Duplicolor. On a summer day in dry Colorado, you can be sanding almost immediately!
I used to get it in the Automotive Dept. at Walmart, but our stores seemed to have dropped paints in Automotive. Seems they now just carry the typical/standard brands of paints like Krylon and Rustoleum in their Paint/Hardware Dept Looks like I'll have to go to the automotive supply shops now.
Has anyone here had good luck with Valspar primer (sanding it or just as a base coat)? The reason I ask is because Valspar (along with Krylon and Rustoleum) are the most common spray paints in my area.
The only Valspar primer I have is JUNK.
Note this is their BASIC (non automotive) primer.
I bought a couple of cans for a buck each on special and quickly found that they were enamel-base not lacquer which means they will take forever to completely dry and NOT sand worth a bucket of warm saliva.
I do not know if Valspar makes an "automotive" type sandable primer.
All I know is their "basic" hardware store primer is hideous.
When in doubt, WHACK the GAS and DITCH the brake !!!
Yes, there is such a thing as NORMAL, if you have to ask what is "NORMAL" , you probably aren't ! Failure may not be an OPTION, but it is ALWAYS a POSSIBILITY.
ALL systems are GO for MAYHEM, AGITATION, CHAOS, TURMOIL, FIASCOS, AGGRAVATION, INSTIGATION, NUISANCE-ACTION, and HAVOC !
I've been considering using primer on my new Estes Saturn V build, but the wrap-arounds are styrene. I believe laquer based primers might mess up the plastic. Am I correct?
Lacquer based primers should not mess up the wraps providing you use them in thin coats with proper drying in between.
Do NOT lay it on thick each coat.
DOPE on the other hand is much hotter than even lacquer and should never be used on styrene.
When in doubt, WHACK the GAS and DITCH the brake !!!
Yes, there is such a thing as NORMAL, if you have to ask what is "NORMAL" , you probably aren't ! Failure may not be an OPTION, but it is ALWAYS a POSSIBILITY.
ALL systems are GO for MAYHEM, AGITATION, CHAOS, TURMOIL, FIASCOS, AGGRAVATION, INSTIGATION, NUISANCE-ACTION, and HAVOC !
The Magnesium Silicate (talc) is at 20%, so theoretically, at least, it should be worth trying as a high-solids primer. Has anyone used it with success?
I have used the Rust Oleum Auto primer you reference above.
It is a "mild" lacquer with a moderate drying time as it has no Acetone in the mix.
Expect a significantly longer than average lacquer drying time, but much faster than enamel.
Sands easily once dry.
When in doubt, WHACK the GAS and DITCH the brake !!!
Yes, there is such a thing as NORMAL, if you have to ask what is "NORMAL" , you probably aren't ! Failure may not be an OPTION, but it is ALWAYS a POSSIBILITY.
ALL systems are GO for MAYHEM, AGITATION, CHAOS, TURMOIL, FIASCOS, AGGRAVATION, INSTIGATION, NUISANCE-ACTION, and HAVOC !
I have used the Rust Oleum Auto primer you reference above.
It is a "mild" lacquer with a moderate drying time as it has no Acetone in the mix.
Expect a significantly longer than average lacquer drying time, butmuch faster than enamel.
Sands easily once dry.
Just make sure if anyone purchases Rust Oleum primer, you get the AUTOMOTIVE version ONLY.
The stuff they sell that is non-automotive is NOT a decent sanding primer; it is more of a base SEALER for the topcoat to be appied onto and will do nothing but clog paper while providing only a MINIMUM of any filling. An added negative bonus of the non-automotive stuff is it is enamel based, which takes forever to dry to boot.
When in doubt, WHACK the GAS and DITCH the brake !!!
Yes, there is such a thing as NORMAL, if you have to ask what is "NORMAL" , you probably aren't ! Failure may not be an OPTION, but it is ALWAYS a POSSIBILITY.
ALL systems are GO for MAYHEM, AGITATION, CHAOS, TURMOIL, FIASCOS, AGGRAVATION, INSTIGATION, NUISANCE-ACTION, and HAVOC !
I do not know if Valspar makes an "automotive" type sandable primer.
All I know is their "basic" hardware store primer is hideous.
Plasti-kote is a Valspar company. P-K seems to focus on the automotive side of things whereas Valspar concentrate on the general home improvement products.
Thank you, foose4string, ghrocketman, and GregGleason! A good "paint formulation sticky" could rate the drying time and "sandability" versus the percentages of petroleum distillates and volatiles (such as acetone and ethylbenzene) versus the solids content. This would enable model rocketeers to select primers and paints based on their chemical constituents instead of by brand, so that those living in areas where only "no-name brands" are available could select good primers and paints with confidence. It would also be helpful to YORF members in other countries where different paint brands may be standard offerings.