It seems that there is now an Elmer's Glue All in new packaging! The applicator is a flat blade sealed spout as opposed to a pin seal. Also seems to be marked with "Interior"
Yup, and it's the "MADE IN USA" version, too. I just picked up a bottle of it yesterday. It was the first bottle of Elmer's Glue-All that I had bought since the waning days of the Clinton administration!
Mark S. Kulka NAR #86134 L1,_ASTRE #471_Adirondack Mountains, NY
Opinions Unfettered by Logic • Advice Unsullied by Erudition • Rocketry Without Pity
Yup, and it's the "MADE IN USA" version, too. I just picked up a bottle of it yesterday. It was the first bottle of Elmer's Glue-All that I had bought since the waning days of the Clinton administration!
But does it grab like the old stuff did? How's it compare to the new stuff and the old stuff?
I tend to discount anything made out of a stack of foam cups.
For any REAL rocket (not oddroc) made out of NORMAL rocketry materials, I stand by my comment about hot melt glue. It IS GARBAGE.
For the one out of a THOUSAND+ available kits on the market, maybe hot melt glue is acceptable.
How 'bout some of that "Liquid Hyde Glue" that has a stink any prankster would be proud to unleash ?
When in doubt, WHACK the GAS and DITCH the brake !!!
Yes, there is such a thing as NORMAL, if you have to ask what is "NORMAL" , you probably aren't ! Failure may not be an OPTION, but it is ALWAYS a POSSIBILITY.
ALL systems are GO for MAYHEM, AGITATION, CHAOS, TURMOIL, FIASCOS, AGGRAVATION, INSTIGATION, NUISANCE-ACTION, and HAVOC !
A representative from Franklin/Titebond returned my call today and was able to discuss the new white glues. The new Translucent Glue is new and the formula is different from the previous all purpose white Glue Titebond used to make. This is the same PVA as Titebond Original except the yellow additive is not added. I thought Yellow glue is Aliphatic, what ever that means. He told me that is the name given to yellow glue but it is a PVA with yellow additive. He did say if I was looking for water resistance than I should use Titebond II, but I don't plan on putting my rockets in the water. I have been using the new Titebond translucent and it dries hard and fast........Sounds like a movie. I did a side by side sanding test with the new glue and yellow glue and there is no difference other than I think the white glue is a little stiffer. As far as shrinking, it shrinks but not as much as the yellow glue.
I just bought a bottle of the new white Molding and Trim glue today and will compare it to the previous Molding and trim glue. The rep said the new version will probably replace the older Molding and Trim Glue since it is a better formula. He said it dries faster, harder and easier to sand. Also he said there is no shrinkage. By the way the previous TMTG is a PVA even though the MSDS call it Thixotropic polyvinyl acetate. Thixotropic just means thickening he said.......Dang big words.
Hmmmm, Just tried the new Trim glue and I cannot tell the difference.
It seems that there is now an Elmer's Glue All in new packaging! The applicator is a flat blade sealed spout as opposed to a pin seal. Also seems to be marked with "Interior"
I HATE those "blade dispensers"... NO control over the glue whatsoever...
They're fine if your coating blocks of wood with glue before clamping them together, but TOTALLY useless for the kind of fine work we do...
I end up robbing "pin seal" caps off old bottles of school glue...
Later! OL JR
The X-87B Cruise Basselope-- THE Ultimate Weapon in the arsenal of Homeland Security and only $52 million per round!
A representative from Franklin/Titebond returned my call today and was able to discuss the new white glues. The new Translucent Glue is new and the formula is different from the previous all purpose white Glue Titebond used to make. This is the same PVA as Titebond Original except the yellow additive is not added. I thought Yellow glue is Aliphatic, what ever that means. He told me that is the name given to yellow glue but it is a PVA with yellow additive. He did say if I was looking for water resistance than I should use Titebond II, but I don't plan on putting my rockets in the water. I have been using the new Titebond translucent and it dries hard and fast........Sounds like a movie. I did a side by side sanding test with the new glue and yellow glue and there is no difference other than I think the white glue is a little stiffer. As far as shrinking, it shrinks but not as much as the yellow glue.
I just bought a bottle of the new white Molding and Trim glue today and will compare it to the previous Molding and trim glue. The rep said the new version will probably replace the older Molding and Trim Glue since it is a better formula. He said it dries faster, harder and easier to sand. Also he said there is no shrinkage. By the way the previous TMTG is a PVA even though the MSDS call it Thixotropic polyvinyl acetate. Thixotropic just means thickening he said.......Dang big words.
Hmmmm, Just tried the new Trim glue and I cannot tell the difference.
Good info there... thanks for that...
"Thixotropic" polyvinyl acetate-- IE "thickened PVA"-- IE thickened white glue... LOL Sounds like all the same stuff to me.
Glad to hear that the TMTG replacement is a bit harder and easier to sand (though I've never had a need to sand it really if you put it on right) but I DID notice it's a bit "softer" than I'd really like to see... sounds like it'll be a good replacement product (not that the original was bad by any stretch-- it's probably THE most impressive new adhesive product I've seen in the last few years!).
I think the Titebond I is the "yellow colored PVA" glue he was talking about correct?? Titebond II is significantly harder, and seems much more like a real "aliphatic resin" glue than a PVA white glue. Of course the differences kinda blur, because they probably just add aliphatic resin to PVA to make yellow wood glue anyway. I use Titebond II on ALL wood/fin joints on my rocket builds, and usually in areas prone to heat soaks, like centering rings to motor tubes. I use white glues to put motor mounts in, to avoid 'sucked in rings' around the body tube from yellow glue shrinkage, and because these joints are not subjected to direct heating anything like the motor tube/centering ring joints are (due to the insulating properties of the centering rings and longer heat soak paths-- IE further from the motor heat source!)
Glad to hear the information you've passed on. Thank you!
OL JR
The X-87B Cruise Basselope-- THE Ultimate Weapon in the arsenal of Homeland Security and only $52 million per round!
I HATE those "blade dispensers"... NO control over the glue whatsoever...
They're fine if your coating blocks of wood with glue before clamping them together, but TOTALLY useless for the kind of fine work we do...
I end up robbing "pin seal" caps off old bottles of school glue...
Later! OL JR
I hear you. When I am making fillets I tape off my fillets....run my finger down the fillet...give it a few minutes and pull the tape off. Works great and you have a very uniform and clean fillet.
I hear you. When I am making fillets I tape off my fillets....run my finger down the fillet...give it a few minutes and pull the tape off. Works great and you have a very uniform and clean fillet.
I thought everyone did fillets that way. They use the same method for epoxy so why not wood glue?
I also use the same method with epoxy clay. Once I get the clay fillet uniform and smooth I pull the tape and then gently blend the edge of the clay into the body tube and fin...after it sets up I come back over it with a piece of sandpaper glued to a wood dowel and then sand it to blend it more.
I thought everyone did fillets that way. They use the same method for epoxy so why not wood glue?
I also use the same method with epoxy clay. Once I get the clay fillet uniform and smooth I pull the tape and then gently blend the edge of the clay into the body tube and fin...after it sets up I come back over it with a piece of sandpaper glued to a wood dowel and then sand it to blend it more.
Since I build LPR, I don't use expoxy on them. I usually follow the directions that come with the kit that would have you run a bead of glue along the joints and smooth out the glue with your finger twice. Then I would use a damp paper towel to wipe away the excess. But the method you described would eliminate a lot of the excess glue.
Since I build LPR, I don't use expoxy on them. I usually follow the directions that come with the kit that would have you run a bead of glue along the joints and smooth out the glue with your finger twice. Then I would use a damp paper towel to wipe away the excess. But the method you described would eliminate a lot of the excess glue.
That's true you wouldn't need any epoxy on LPR kits...I do use the epoxy on the kits for engine mount and coupler installation.
Comment