    I thought I'd check the knowledge base around here . . . .

    I purchased on old Estes Avenger on eBay for $5 for rebuild. The fins were off and the nose was missing. I happened to still have my Avenger nose from when I was a kid. I don't mind doing restoration work, so I started in on this oldie.

    With patience, I was able to remove the engine mounts and the staging coupler. As I began to work on the booster fins I noticed the paint was flaking off. Upon closer inspection, I realized that it wasn't just the paint but the glassine layer on the tube itself. And it wasn't just on the booster - - the sustainer tube also had the same problem.

    Now, there are a couple of things that lead me to believe this was an older, possibly pre-Damon kit: 1) the shock cord was threaded through the body tube and painted over like on a similar vintage X-ray; 2) the launch lug was on a dowel stand-off rather than glued directly to the body as on the Damon-era kits I built as a kid.; and 3) the quality of the mounting rings on the engine mounts is very poor.

    So the question is: Has anybody else experienced flaking or separating glassine on older body tubes?
    NAR 79743
    NARTrek Silver
    I miss being SAM 062

    Awaiting First Launch: Too numerous to count
    Finishing: Zooch Saturn V; Alway/Nau BioArcas;
    Repair/Rescue: Cherokee-D (2);
    On the Bench: 2650; 2X Nike-Ram
    Dream Stage: 1/39.37 R-7
  • mwtoelle
    Flying since 1977
    • Oct 2010
    • 491
    • Middle TN

    #2
    I had a Warp II kit with an extra layer of glassine on the booster body tube. The annoying thing about it is that I had already glued on the fins. The shock cord on your Avenger was probably a replacement. The original kit used the trifold shock cord mount. The 1/12" dowel underneath the launch was to allow the rocket to use the Estes C-Rail. The flat centering rings were pretty thin (about the thickness of 2-3 index cards) until sometime in the 1980s when they started using 0.050" stock.
    'Til next time,

    Mike Toelle

    NAR 31692 L1

    SAM 0373

    Comment

    • Stargate
      Intermediate Rocketeer
      • May 2011
      • 50

      #3
      I have one or 2 thick walled Airframe tubes here ( something between a BT-55 and BT-60) size that are made entirely of Glassine layers, These were used in making rockets for Lightening research.