    White glue stinks for attaching Nomex.
    I'd use CA or high-temp epoxy such as J-B Weld to attach it. Then again, I'd just use hi-temp J-B Weld without the Nomex for flameproofing
    When in doubt, WHACK the GAS and DITCH the brake !!!

    Yes, there is such a thing as NORMAL
    , if you have to ask what is "NORMAL" , you probably aren't !

    Failure may not be an OPTION, but it is ALWAYS a POSSIBILITY.
    ALL systems are GO for MAYHEM, AGITATION, CHAOS, TURMOIL, FIASCOS, AGGRAVATION, INSTIGATION, NUISANCE-ACTION, and HAVOC !

    Comment

    • Coconuteater64
      Grumpy Old Man
      • Oct 2015
      • 48
      • Between Chattanooga and Atlanta, where the "yee" meets the "haw"

      #17
      Originally posted by sandman
      Carl McLawthorn told about the motor testing he did and he told me Estes engines shoot out a healthy flame for more than a few seconds AFTER the ejection charge fires.

      This is like a mini blow torch the evidence of that is especially evident if you ever had to rebuild a Fliskits Duece's Wild.

      The blast of the two angled motors really do a number on the body tube.
      Well, that explains a lot! I have a Quest kit (no idea of the name, my kids brought it home from scout camp for me) that I modified to eject the fin can rather than the nose cone. It's got over 40 flights and it's still going strong. My Mark II clone burned out in a half dozen flights. Both are minimum diameter rockets. Sounds plausible.

      Comment

      • olDave
        Craftsman
        • Sep 2015
        • 183
        • west Ft Worth

        #18
        reinforcements

        -swab area ahead of thrust ring with epoxy
        -swab area ahead of thrust ring with C/A
        -swab area ahead of thrust ring with white or yellow glue
        -add coupler (as already posted above)....better than any of above approaches
        -use extra short piece of BT, slit side, collapse diameter slightly, use in place of coupler idea
        -spray inside of BT ahead of thrust ring with grill paint or motor block paint (high temperature paint)
        -find roll of sheet alum, or steel, tape/film (local hdwre store), snip appropriate-sized piece, roll to compress, insert into position ahead of thrust ring, etc.....piece of alum sheet from favorite beverage container might be substituted

        Keep in mind that you are protecting against HEAT more so than temperature, and almost any mass you add to harden/reinforce the local BT will also add mass that helps protect the BT. The added liner material must be raised to the temps where the BT begins to char before any damage occurs, and the mass of the added liner slows down this absorbtion of heat.
        NAR 20602
        used to be "powderburner" in another life

        Comment

        • jeffyjeep
          Old Submariner
          • Jan 2009
          • 8465
          • Home of Wayne & Garth

          #19
          Originally posted by gpoehlein
          When I was a kid (a VERY long time ago) I had a large Gilbert Chemistry set. Adding to it with Perfect chemicals and labware, I ended up with a rather impressive lab in my parent's basement. Mind you, this was back in the 60s when a Chemistry set was a REAL chemistry set.

          Anyway, one of the chemicals that came with the set was Sodium Silicate, or waterglass. This stuff was incredible as a fire retardant - much better than Boric Acid. Of course, this stuff is not available any more (I could go on a serious rant about the strongest chemical in a home chemistry set today is vinegar, and you have to provide that - but I digress). I came across an article a while back that tells how to convert the pellets inside those silicone drying packs into sodium silicate. I;m pretty sure the article was on Make.com. You could always make some and paint that on the inside of your model - enough will soak into the cardboard that it should make it pretty much fireproof.

          <Edit> I did a bit of searching on Google and discovered that you should be able to purchase sodium silicate at Lowes, Home Depot, Menards, or any other hardware store - it is also used to coat concrete surfaces to waterproof them. Also, I had forgotten that waterglass was traditionally used to preserve fresh eggs - you can dip a clean fresh egg in waterglass solution and it will remain edible for over a year without refrigeration!
          I don't intend to hijack this thread--but you're right about the eggs. We would get large crates of eggs aboard the sub before we "went north" and they would last for several weeks without refrigeration while we were under the polar ice cap.
          Never trust an atom. They make up everything.

          4 out of 3 people struggle with math.

          Chemically, alcohol IS a solution.

          NAR# 94042
          SAM# 0078

          Comment

          Working...