Originally posted by tbzep
before... Choose hard C-grain balsa if possible. A-grain is just asking for trouble anyway.
1. apply it BEFORE attaching to rocket
2. use it full strength and apply it with your finger (vinyl or nitrile glove recommended). rub it in.
3. apply it on both sides at roughly the same time (i.e. not one side and let dry, then other side)
from what I can tell in the picture, your fins were close to A-grain, and your F'n'F had a much higher water content than it needed to be.

) Because of that, I mainly just use it on nose cones. But this stuff is truly great, and it is what I would use all the time, if I could get it in larger bottles. The Delta Ceramcoat filler and Pine-Pro are both water-based, but I have never had either one cause fin warping. They both just clean off my brushes with soap and water. Before you wet-sand either one, though, make sure that the coat has completely dried.

. I haven't tried make fins from 1/32" birch plywood yet, but it might work out that the slight extra weight would be offset by the much thinner aerodynamic cross-section.