Originally posted by scigs30
I usually start with 400-grit aluminum oxide paper. This grade (grit count) of paper is usually reserved for the final stages of sanding, but I find that it works really well for this particular purpose too. The idea is not to really sand the coating down, but more to smooth it off. I find that I get the best results when there is enough water on the paper to create a bit of very loose slurry on the surface as I sand. After anywhere from 30 seconds to a minute of sanding, I stop and wipe the cone dry with a paper towel, and check my progress. Usually, two or three coats of Ceramcoat, with wet-sanding between coats, is enough. Since I am usually going for a mirror finish, though, I tend to keep on applying thin coats and wet-sanding until I reach a point of diminishing returns. This extra work is a bit of a pain, but I am almost always pleased with the results, so for me it is worth the additional effort. Your mileage and your priorities may vary, though. One thing that I learned from reading Micromeister's Tech Tips a long time ago was that the smoother you get the base layer, the smoother your topcoat will be.
Better than Delta Ceramcoat APS by a mile is Pine-Pro Sanding Sealer, as I mentioned in an earlier post. It looks similar, but it is thicker and it fills the grain faster, it dries harder, and it wet-sands smoother than the Delta product. The only size that I can find it in is a 2 oz. bottle at my "local" hobby shop, which is 52 miles away. The LHS usually has only one bottle in stock (sometimes two), so that's all I can get per trip. Sadly, a single 2 oz. bottle doesn't last long. If only I could stock up on the stuff, I would be using it for all of my wood surface prep.
Mark \\.

) As I mentioned, the reason that you would do better to wet-sand this particular product rather than dry-sanding it is because wet-sanding avoids overheating the sealer and it makes the sanding go much easier (and quicker, too). I tried sanding it in the usual way at first, but I kept experiencing the softening and gumming problems that I described, so I switched to wet-sanding it, which worked much better.
Comment