Balsa Finishing?

Collapse
X
 
  • Time
  • Show
Clear All
new posts
  • Mark II
    Forest Sprite
    • Dec 2006
    • 3657
    • Back Up in the Woods

    #16
    Another vote for using laminating epoxy on balsa nose cones. For anything smaller than BT-50 I use it exclusively. For BT-55 to ST-18 (1.84") I first soak the wood as best I can with Minwax Wood Hardener. Wood Hardener seals but does not fill the grain but as the name indicates, it toughens up the wood. I let the hardener in the outer layers of wood cure for a couple of days, then lightly sand it and apply another treatment of MWH. After that, I hang it up for up to a couple of weeks to allow the hardener to fully cure inside and out. (The surface can feel dry and hard while the inner layers of wood are still uncured and soft.) I sand it again to get the roughness out after it cures, and then coat the cone with laminating epoxy as before. For large balsa cones, (2" and up) I usually just use Wood Hardener alone. The larger the cone, the longer it can take to cure, so I set it aside for awhile. I don't build fast, so this isn't a problem for me.

    Large balsa cones tend to be quite smooth, at least the ones that I get typically are. Sanding the fully-cured hardened wood takes care of nearly all of the raised grain. Large cones can take up to a month, sometimes longer, to fully cure after a couple of treatments with wood hardener, but the result is worth the wait. Factor that into your timeline for completing the project. I apply some Delta Ceramcoat All-Purpose Sealer to fill in little pores or remaining grain. This sealer works well but isn't quite as hard as epoxy. It is easier than mixing up a bucket full of epoxy, though and the MWH has already done a very good job of making the wood dent-resistant.

    If there are any problem areas on the bigger cones, I apply Aeropoxy Lightweight Filler to them. This is a two-part epoxy-based wood filler. It can be sanded fairly easily after it cures, but it fills the gaps or holes with very tough material, the hardest wood filler that I have ever used (including Dap Plastic Wood). For smaller nose cones, I fix any remaining problem areas with either Carpenter's Wood Filler or Bondo Spot and Glazing Putty. I may also use the aforementioned plastic wood for this, too, on small cones, but otherwise I reserve my plastic wood for repairing nicks, cuts and sanding errors in the edges of balsa fins. It is truly superb for that particular job.

    For fins, I use either of two methods that have already been mentioned. Especially with small-pattern fins, I fill and seal them with Aerogloss products in the same manner that ghrocketman described. With larger, broader fins, I paper the balsa. I have had excellent results with using Reynold Freezer Paper for this. The paper resembles white butcher paper, but it has a thin and very smooth coating of plastic on one side. I use a craft stick or a plastic (Bondo) putty spreader to apply a thin, even coating of white glue to the uncoated side of the paper and then bond it to the fin. As soon as I do one side, I follow up as quickly as possible by papering the other side in order to minimize warping. I lay all of the fins on a sheet of wax paper on my smooth Formica counter or on a smooth table, cover them with another sheet of wax paper, and then pile a stack of smooth textured hardcover books on them. Since there's not much air circulation under the books, I give the fins 24 to 48 hours to get fully dry. I want them to be completely dry so that they won't develop any slight warps after I remove them from the press. I only use white glue for this, since it shrinks much less than wood glue. The plastic side of the freezer paper is primer-ready without any further preparation.
    Mark S. Kulka NAR #86134 L1,_ASTRE #471_Adirondack Mountains, NY
    Opinions Unfettered by Logic • Advice Unsullied by Erudition • Rocketry Without Pity
    +09281962-TAK-08272007+
    SAM # 0011

    Comment

    • ghrocketman
      President, MAYHEM AGITATORS, Inc.
      • Jul 2005
      • 15964
      • Nunya Bizznuss, Michigan

      #17
      Yes, that Dap/Red Devil grainy stuff in the can/tube which is powdered cellulose in a paste form mixed with Acetone and Toluene.
      If you add some of that to the Talc dissolved in the clear dope, it fills even better.
      Just don't add too much; like Cayenne Pepper, a little goes a LONG way.

      ANY process that takes even a WEEK (let alone a month) to dry, I immediately dismiss as taking WAAAAYYYY too stinkin' long.
      I'd sooner shoot Imron out of a NON-HVLP paint gun WITHOUT a fresh-air breathing supply before I would use any finishing materials that have any step resembling "wait a month for drying"
      When in doubt, WHACK the GAS and DITCH the brake !!!

      Yes, there is such a thing as NORMAL
      , if you have to ask what is "NORMAL" , you probably aren't !

      Failure may not be an OPTION, but it is ALWAYS a POSSIBILITY.
      ALL systems are GO for MAYHEM, AGITATION, CHAOS, TURMOIL, FIASCOS, AGGRAVATION, INSTIGATION, NUISANCE-ACTION, and HAVOC !

      Comment

      • Mark II
        Forest Sprite
        • Dec 2006
        • 3657
        • Back Up in the Woods

        #18
        Originally posted by ghrocketman
        ANY process that takes even a WEEK (let alone a month) to dry, I immediately dismiss as taking WAAAAYYYY too stinkin' long.
        I'd sooner shoot Imron out of a NON-HVLP paint gun WITHOUT a fresh-air breathing supply before I would use any finishing materials that have any step resembling "wait a month for drying"


        Well, I did say that I usually took my time when I build. But occasionally even I think that some of my waiting times are excessive. Minwax Wood Hardener does seem to need the time, though and I put up with it because it really really toughens up the balsa. I pay enough for balsa nose cones, so I want to make sure that they are reasonably durable. I have a 9.7" long, 2.34" dia. balsa nose cone that has survived more drops and falls (from up to 5 feet in height tip first onto a hard floor) than you can whip a launch rod at, and yet the worst damage that it has sustained are a couple of very small and superficial dings. So yeah, the long cure time can be a pain, but the ultimate results are amazing. I should point out that smaller nose cones don't take anywhere near as long to fully cure after the treatment. The really long cure times (on the scale of weeks) are for very large balsa nose cones. They are more costly to replace, though, so they are the ones that you really want to protect.
        Mark S. Kulka NAR #86134 L1,_ASTRE #471_Adirondack Mountains, NY
        Opinions Unfettered by Logic • Advice Unsullied by Erudition • Rocketry Without Pity
        +09281962-TAK-08272007+
        SAM # 0011

        Comment

        • ghrocketman
          President, MAYHEM AGITATORS, Inc.
          • Jul 2005
          • 15964
          • Nunya Bizznuss, Michigan

          #19
          Soaking the cones with a good penetrating coat of 30+ minute pot-life epoxy would do the same though, dontcha think ??
          It would fully cure in a DAY, not a month.
          If I let a project sit for a month, I lose interest in it usually.
          When in doubt, WHACK the GAS and DITCH the brake !!!

          Yes, there is such a thing as NORMAL
          , if you have to ask what is "NORMAL" , you probably aren't !

          Failure may not be an OPTION, but it is ALWAYS a POSSIBILITY.
          ALL systems are GO for MAYHEM, AGITATION, CHAOS, TURMOIL, FIASCOS, AGGRAVATION, INSTIGATION, NUISANCE-ACTION, and HAVOC !

          Comment

          • Mark II
            Forest Sprite
            • Dec 2006
            • 3657
            • Back Up in the Woods

            #20
            Originally posted by ghrocketman
            Soaking the cones with a good penetrating coat of 30+ minute pot-life epoxy would do the same though, dontcha think ??
            It would fully cure in a DAY, not a month.
            If I let a project sit for a month, I lose interest in it usually.
            As I wrote earlier, I do in fact use laminating epoxy on many of my nose cones. I tend to use the wood hardener mostly on the really big ones. They are the most expensive, and they need all the hardening that I can give them, so I pull out all of the stops when I build with them. Needless to say, these are for my big projects, which are only a small portion of what I build. And as I have also already mentioned twice now, the cure time for wood hardener on smaller nose cones is much shorter than that.

            The laminating epoxy that I use does indeed soak easily, at least for a little way, into the wood. I usually give it as many as three coatings, sanding it down after each one. It cures hard in several hours, but I usually wait until the next day to sand it. It certainly helps, but it doesn't make them totally bomb-proof. I've had things puncture through the epoxy a couple of times. The coating can only do so much when the wood underneath it is soft. So far I have only used BSI 20 Minute Finish Cure epoxy on nose cones. If I did it with West Systems or Aeropoxy laminating epoxy, the coating might be even harder. I do use long-cure epoxy for structural adhesion, but I'd be afraid that it would be too hard to sand if I coated a nose cone with it.

            I'm not saying that my method is the only way or necessarily the best way; I posted about it because it is my own way. I have used a number of other methods for filling and sealing nose cones before this, so I know how they go. One that I haven't, though, is the dope augmented with talc and a little plastic wood method that you described above. It looks interesting and is one that I'll have to investigate sometime.
            Mark S. Kulka NAR #86134 L1,_ASTRE #471_Adirondack Mountains, NY
            Opinions Unfettered by Logic • Advice Unsullied by Erudition • Rocketry Without Pity
            +09281962-TAK-08272007+
            SAM # 0011

            Comment

            • ghrocketman
              President, MAYHEM AGITATORS, Inc.
              • Jul 2005
              • 15964
              • Nunya Bizznuss, Michigan

              #21
              I was speaking of using structural, NOT laminating, epoxy to harden cones.
              Good stuff like Aeropoxy or West System, NOT 50/50 hobby shop stuff that is loaded with fillers to make the mix even for those too challenged to use measuring cups.
              REAL epoxy is far stronger than hobby store stuff, which is not all that bad.

              My method of 3 coats balsa fillercoat followed by 2+ of Sanding Sealer will not result in a cone anywhere near as hard as an epoxy coated one. Mine look great but are a bit fragile. They will NOT survive bouncing off pavement without mangle marks. Then again, I dont do that to them.
              When in doubt, WHACK the GAS and DITCH the brake !!!

              Yes, there is such a thing as NORMAL
              , if you have to ask what is "NORMAL" , you probably aren't !

              Failure may not be an OPTION, but it is ALWAYS a POSSIBILITY.
              ALL systems are GO for MAYHEM, AGITATION, CHAOS, TURMOIL, FIASCOS, AGGRAVATION, INSTIGATION, NUISANCE-ACTION, and HAVOC !

              Comment

              • Solomoriah
                Incorrigible Kit Basher
                • Jul 2006
                • 1940
                • USA

                #22
                I've been getting darn good results by brushing thinned FnF over the fins and cone, sanding when dry, then priming and sanding with a dry-sand compatible spray primer. Doesn't make my eyes water, and it's cheap.
                NAR # 115523
                Once upon a better day... SAM #0076
                My site: http://rocketry.gonnerman.org

                Comment

                • Mark II
                  Forest Sprite
                  • Dec 2006
                  • 3657
                  • Back Up in the Woods

                  #23
                  Originally posted by ghrocketman
                  I was speaking of using structural, NOT laminating, epoxy to harden cones.
                  Good stuff like Aeropoxy or West System, NOT 50/50 hobby shop stuff that is loaded with fillers to make the mix even for those too challenged to use measuring cups.
                  REAL epoxy is far stronger than hobby store stuff, which is not all that bad.
                  Well then, we're more or less in agreement. I want to do that - apply something like a thin formulation of West System epoxy to some nose cones. I think you're right, they'll be much harder than they are with the epoxy that I use now. Being able to sand them smooth is going to be deal maker or deal breaker, but West Systems is known for their large assortment of additives and modifiers, so maybe they'll have something that I can add in to make it easier to sand without significantly weakening it. If it will penetrate well, that will be a bonus too, because it will help somewhat the issue of a soft wood core inside a thin hard shell. Otherwise once something gets through the armor, it has no protection. Toughening up the wood itself in addition to installing body armor is ultimately the best choice if you are going to use balsa, but the most effective and widely available method for doing that takes some time to do the job.

                  Let me reiterate yet again though that the longer cure times seem to be a factor only with large (e.g., BT-70, BT-80, etc.) balsa cones. With smaller cones, the wait should not be longer than a week at the most, and often more like 2 or 3 days or less. That doesn't seem like an excessive cure time. Many of us wait for similar intervals between paint colors. The builder doesn't have to use wood hardener, of course, but my own anecdotal experience indicates that it is highly effective.
                  Mark S. Kulka NAR #86134 L1,_ASTRE #471_Adirondack Mountains, NY
                  Opinions Unfettered by Logic • Advice Unsullied by Erudition • Rocketry Without Pity
                  +09281962-TAK-08272007+
                  SAM # 0011

                  Comment

                  • jetlag
                    Old BAR
                    • Aug 2006
                    • 2294

                    #24
                    I like to use thin CA to harden/toughen up cones when I feel the need. Works well for overly soft fins, as well, like the wood that comes in The Launch Pad kits. And the weight penalty is minimal if not nil.
                    I use epoxy for everything else, though. Holds up a lot better than white/wood glues, especially in the heat we have here. Fins don't sag if the rocket is left on its side.
                    Works for me!
                    A-

                    Comment

                    • luke strawwalker
                      BAR
                      • Dec 2007
                      • 6151
                      • Needville and Shiner, TX

                      #25
                      Originally posted by Solomoriah
                      I've been getting darn good results by brushing thinned FnF over the fins and cone, sanding when dry, then priming and sanding with a dry-sand compatible spray primer. Doesn't make my eyes water, and it's cheap.
                      Yeah, I agree...

                      I mean, to each his own, if it works for you and you enjoy it go for it, but looking at some of the prices folks have talked about for these sanding sealers and dope and stuff, and the fumes and difficulty in using them, and all that, I'm convinced that I can achieve the same results at less cost and with equal durability and finish with far cheaper and less volatile materials...

                      BUT, that said, I've never tried the sealer/dope methods either, so I admit that other folks see the benefit of it...

                      I personally have never seen the need. My results are good enough, especially for LPR. HPR, the other stuff might be called for. I dunno-- no interest in HPR.

                      Later! OL JR
                      The X-87B Cruise Basselope-- THE Ultimate Weapon in the arsenal of Homeland Security and only $52 million per round!

                      Comment

                      • ghrocketman
                        President, MAYHEM AGITATORS, Inc.
                        • Jul 2005
                        • 15964
                        • Nunya Bizznuss, Michigan

                        #26
                        Using Balsa Fillercoat and Sanding Sealer has the CORRECT, nostalgic, YE OLDE aroma for building VINTAGE designs.
                        It has the added benefit that it does not turn the shop into a friggin dust bowl everytime you get a piece of sandpaper within a yard of touching balsa coated with it, unlike Fill-n'-Finish that immediately generates an atom-bomb's worth of dust the second you touch it with any sanding material.
                        I have less use for ANY water-based finishing material than I have for taking a hot brandin' iron to a dodge-bawl match.
                        When in doubt, WHACK the GAS and DITCH the brake !!!

                        Yes, there is such a thing as NORMAL
                        , if you have to ask what is "NORMAL" , you probably aren't !

                        Failure may not be an OPTION, but it is ALWAYS a POSSIBILITY.
                        ALL systems are GO for MAYHEM, AGITATION, CHAOS, TURMOIL, FIASCOS, AGGRAVATION, INSTIGATION, NUISANCE-ACTION, and HAVOC !

                        Comment

                        • Mark II
                          Forest Sprite
                          • Dec 2006
                          • 3657
                          • Back Up in the Woods

                          #27
                          When I opened a bottle of Aerogloss dope for the first time after becoming a BAR, I had a Proustian moment. I was instantly transported back to the basement of my house in Grand Rapids. All of the cares and regrets of my adult life vanished (temporarily). It was late spring, 1967, I was 13 years old, and I was painting my Astron Alpha, my very first model rocket. Ahh, good times, good times....

                          To me, that's the real deal, the authentic experience.

                          I too am hesitant about putting anything as watery as thinned Carpenter's Wood Filler onto raw balsa.

                          A few weeks ago, someone over on TRF started a thread about brushing his balsa fins with Bondo Glazing and Spot Putty. He used acetone to thin it to brushable consistency. I didn't follow the entire thread but apparently he obtained good results with this technique. I have not tried this myself yet, so don't interpret my mention of it as a personal endorsement.
                          Last edited by Mark II; 03-11-2011, 10:35 PM.
                          Mark S. Kulka NAR #86134 L1,_ASTRE #471_Adirondack Mountains, NY
                          Opinions Unfettered by Logic • Advice Unsullied by Erudition • Rocketry Without Pity
                          +09281962-TAK-08272007+
                          SAM # 0011

                          Comment

                          • Solomoriah
                            Incorrigible Kit Basher
                            • Jul 2006
                            • 1940
                            • USA

                            #28
                            Hey, I've been using water-thinned FnF for a long time with good results.

                            The only warning I can give you is to coat both sides evenly at the same time. The only time I've seen warping is when I've not followed that rule.
                            NAR # 115523
                            Once upon a better day... SAM #0076
                            My site: http://rocketry.gonnerman.org

                            Comment

                            • Mark II
                              Forest Sprite
                              • Dec 2006
                              • 3657
                              • Back Up in the Woods

                              #29
                              Luke, I started out using simple techniques, too, and I still use them in some builds. I got into using more "exotic" techniques to address certain specific issues. Eventually I found that some of them were broadly applicable, and so they became part of my regular toolkit of techniques. I previously mentioned using Delta Ceramcoat All-Purpose Sealer. If you really want to keep things simple, just brush three to four coats of this product onto the balsa. Sand between coats. For a silky smooth final surface, gently wet-sand the final coat with 400 or 600 grit aluminum oxide sandpaper (the black kind). The product has no obnoxious fumes and does not irritate or soak readily into skin, so it can be safely used by children. You can buy it at many craft stores, including Michaels, A. C. Moore and Joanne's Fabrics. It is in the tole painting section.

                              An even better product in my opinion, and probably the best product of its kind, is Pine Pro Sanding Sealer. Both products fill the grain and seal the wood at the same time, performing two finishing steps with one product. But Pine Pro does a noticeably better job of it, going on more easily with a paint brush, requiring fewer coats to completely fill the grain, sanding smoother and producing a harder surface. The only problem with it is that it only comes in 2 oz. bottles, which don't last long. I can easily kill from one-half to one entire bottle on the nose cone and fins of a BT-20 or BT-50-sized 3FNC rocket. So you have to keep buying it and buying it. You can get the Delta product in quantities up to 12 oz., which is much handier. I reserve Pine Pro for my high-value clones that I want to exhibit that "catalog pic" look. Wet sanding the final coat also produces a glass-smooth surface, even better than with the Delta product. And just as with the Delta sealer, Pine Pro has no unpleasant fumes, does not irritate skin (as far as I can tell) and can be safely used in classes and by Scout groups. This product can be found in hobby shops; look in the section that has the parts for pinewood derby cars.

                              Neither product produces a particularly durable or nick-resistant coating on the wood (more important for nose cones than for fins), but what you lose in hardiness you gain in simplicity. And if you are working with kids, these are the products to use. Neither one requires any special technique to apply - just brush the product on in even coats, using a synthetic bristle paint brush (so you don't leave hairs in the coat). Both products clean up easily with water and a little bit of soap. Make sure that you clean your brushes while they are still wet, because once either product dries onto the bristles, you'll never get it out.
                              Last edited by Mark II; 03-11-2011, 10:08 PM.
                              Mark S. Kulka NAR #86134 L1,_ASTRE #471_Adirondack Mountains, NY
                              Opinions Unfettered by Logic • Advice Unsullied by Erudition • Rocketry Without Pity
                              +09281962-TAK-08272007+
                              SAM # 0011

                              Comment

                              • luke strawwalker
                                BAR
                                • Dec 2007
                                • 6151
                                • Needville and Shiner, TX

                                #30
                                Originally posted by ghrocketman
                                I have less use for ANY water-based finishing material than I have for taking a hot brandin' iron to a dodge-bawl match.
                                YEE-HAW!!!!!

                                Or should I say HEE-HAW?? Going kinda redneck on us GH?? LOL (ducks and runs)



                                Later! OL JR
                                The X-87B Cruise Basselope-- THE Ultimate Weapon in the arsenal of Homeland Security and only $52 million per round!

                                Comment

                                Working...