    Originally posted by Mark II
    Luke, I started out using simple techniques, too, and I still use them in some builds. I got into using more "exotic" techniques to address certain specific issues. Eventually I found that some of them were broadly applicable, and so they became part of my regular toolkit of techniques. I previously mentioned using Delta Ceramcoat All-Purpose Sealer. If you really want to keep things simple, just brush three to four coats of this product onto the balsa. Sand between coats. For a silky smooth final surface, gently wet-sand the final coat with 400 or 600 grit aluminum oxide sandpaper (the black kind). The product has no obnoxious fumes and does not irritate or soak readily into skin, so it can be safely used by children. You can buy it at many craft stores, including Michaels, A. C. Moore and Joanne's Fabrics. It is in the tole painting section.

    An even better product in my opinion, and probably the best product of its kind, is Pine Pro Sanding Sealer. Both products fill the grain and seal the wood at the same time, performing two finishing steps with one product. But Pine Pro does a noticeably better job of it, going on more easily with a paint brush, requiring fewer coats to completely fill the grain, sanding smoother and producing a harder surface. The only problem with it is that it only comes in 2 oz. bottles, which don't last long. I can easily kill from one-half to one entire bottle on the nose cone and fins of a BT-20 or BT-50-sized 3FNC rocket. So you have to keep buying it and buying it. You can get the Delta product in quantities up to 12 oz., which is much handier. I reserve Pine Pro for my high-value clones that I want to exhibit that "catalog pic" look. Wet sanding the final coat also produces a glass-smooth surface, even better than with the Delta product. And just as with the Delta sealer, Pine Pro has no unpleasant fumes, does not irritate skin (as far as I can tell) and can be safely used in classes and by Scout groups. This product can be found in hobby shops; look in the section that has the parts for pinewood derby cars.

    Neither product produces a particularly durable or nick-resistant coating on the wood (more important for nose cones than for fins), but what you lose in hardiness you gain in simplicity. And if you are working with kids, these are the products to use. Neither one requires any special technique to apply - just brush the product on in even coats, using a synthetic bristle paint brush (so you don't leave hairs in the coat). Both products clean up easily with water and a little bit of soap. Make sure that you clean your brushes while they are still wet, because once either product dries onto the bristles, you'll never get it out.
    Thanks for the tips... Good stuff!

    The one thing I've learned in life is that there is, most of the time, more than one way to skin a cat... What works (best) for one person doesn't necessarily work best for someone else. BUT, we can ALL learn something from each other, and that's the important thing.

    I hope neither you nor GH took anything I said as disrespectful. It wasn't intended that way. I was just agreeing with Solomoriah, that the 'water based' methods we've been using work "just as well" as these other methods seem to be working for you guys, and the cost, time, and work seems lower as well. BUT, as GH pointed out, it DOES produce some dust... (not an "atom bomb's worth" though-- I don't have a workshop (I took over the dining room table and do most of my sanding there or in the living room watching TV... the main way to reduce the dust, is DON'T PUT AN INCH THICK LAYER OF FNF ON STUFF-- that way there's not that much to sand off

    At any rate, to each his own, and let's all have fun and agree to disagree...

    Respects! OL JR
    The X-87B Cruise Basselope-- THE Ultimate Weapon in the arsenal of Homeland Security and only $52 million per round!

    Comment

    • Solomoriah
      Incorrigible Kit Basher
      • Jul 2006
      • 1940
      • USA

      #32
      I don't mind the dust, since I can't sand indoors anyway. My daughter is allergic to dust. And yeah, you don't put that much on in the first place, and you don't get that much off when you sand it.

      GH just likes to rant... it's part of his charm.
      NAR # 115523
      Once upon a better day... SAM #0076
      My site: http://rocketry.gonnerman.org

      Comment

      • Mark II
        Forest Sprite
        • Dec 2006
        • 3657
        • Back Up in the Woods

        #33
        Originally posted by luke strawwalker
        I hope neither you nor GH took anything I said as disrespectful. It wasn't intended that way.
        Not at all. The purpose of this thread is to share our different techniques. We all have our own, and most of us have more than one in our bag of tricks. I learn about new approaches to doing things by talking to other builders, so I get as much out of threads like these as the original posters do. When I posted my response to you, it wasn't to criticize but rather to explain. But in addition, you and Solo prompted me to recall the other techniques that I described further on. I hadn't thought to mention them until I read both of your posts.
        Mark S. Kulka NAR #86134 L1,_ASTRE #471_Adirondack Mountains, NY
        Opinions Unfettered by Logic • Advice Unsullied by Erudition • Rocketry Without Pity
        +09281962-TAK-08272007+
        SAM # 0011

        Comment

        • Mark II
          Forest Sprite
          • Dec 2006
          • 3657
          • Back Up in the Woods

          #34
          Originally posted by luke strawwalker
          BUT, as GH pointed out, it DOES produce some dust... (not an "atom bomb's worth" though-- I don't have a workshop (I took over the dining room table and do most of my sanding there or in the living room watching TV... the main way to reduce the dust, is DON'T PUT AN INCH THICK LAYER OF FNF ON STUFF-- that way there's not that much to sand off

          At any rate, to each his own, and let's all have fun and agree to disagree...

          Respects! OL JR
          Oh see, I DO know what he's talking about there. I try to be careful about how much filler I put on because I'm mindful of how much I'll have to sand off later, but still I wind up with a good layer of dust over myself and everything else in the vicinity by the time I'm done sanding. I get it regardless of whether I use Carpenter's Wood Filler or Bondo Glazing and Spot Putty or Aeropoxy Light Filler. That's why I prefer to go outdoors to sand down filler - I don't have to clean up the immediate surroundings afterward. I think I mentioned that I do like to use dope filler and sanding sealer on small balsa parts, particularly fins, but that gets to be too expensive once the parts get bigger. Using the other fillers is much less expensive for large areas, so I put up with the dust. And besides, I use CWF and Bondo putty far more often to fill in tube spirals than for anything else, and dope-based products just won't work in that situation.
          Mark S. Kulka NAR #86134 L1,_ASTRE #471_Adirondack Mountains, NY
          Opinions Unfettered by Logic • Advice Unsullied by Erudition • Rocketry Without Pity
          +09281962-TAK-08272007+
          SAM # 0011

          Comment

          • ghrocketman
            President, MAYHEM AGITATORS, Inc.
            • Jul 2005
            • 15964
            • Nunya Bizznuss, Michigan

            #35
            No offense taken whatsoever.
            By the way, "bondo" spot and glazing putty is sort of "dope based" as the same thinners (Toluene and Acetone) for dopes are the solvent base for that putty.
            One can make a very good brushable balsa fillercoat by thinning one part bondo putty to four parts dope thinner. It will however produce almost as much dust as water-base F-n-F.
            When in doubt, WHACK the GAS and DITCH the brake !!!

            Yes, there is such a thing as NORMAL
            , if you have to ask what is "NORMAL" , you probably aren't !

            Failure may not be an OPTION, but it is ALWAYS a POSSIBILITY.
            ALL systems are GO for MAYHEM, AGITATION, CHAOS, TURMOIL, FIASCOS, AGGRAVATION, INSTIGATION, NUISANCE-ACTION, and HAVOC !

            Comment

            • luke strawwalker
              BAR
              • Dec 2007
              • 6151
              • Needville and Shiner, TX

              #36
              Originally posted by ghrocketman
              No offense taken whatsoever.
              By the way, "bondo" spot and glazing putty is sort of "dope based" as the same thinners (Toluene and Acetone) for dopes are the solvent base for that putty.
              One can make a very good brushable balsa fillercoat by thinning one part bondo putty to four parts dope thinner. It will however produce almost as much dust as water-base F-n-F.
              Yes, that's true... but nothing I've found fills a tube spiral as good as Bondo Spot Putty... I've heard folks use FNF for that, and I've tried, but it seems that as soon as I sand the stuff off, it ALL seems to be gone, and the tube spiral is just as much there as when I started. I even tried two applications one time and STILL had spiral left, so I just went back to the BSP... one app, sand, done.

              I usually just wipe/daub the stuff on with a bare finger (probably not the brightest idea, but oh well, SOMETHING's gonna kill me sooner or later anyway) and it's quick and easy. Only downside is you get the "funky pink finger" LOL

              later! OL JR
              The X-87B Cruise Basselope-- THE Ultimate Weapon in the arsenal of Homeland Security and only $52 million per round!

              Comment

              • Mark II
                Forest Sprite
                • Dec 2006
                • 3657
                • Back Up in the Woods

                #37
                Originally posted by luke strawwalker
                Yes, that's true... but nothing I've found fills a tube spiral as good as Bondo Spot Putty... I've heard folks use FNF for that, and I've tried, but it seems that as soon as I sand the stuff off, it ALL seems to be gone, and the tube spiral is just as much there as when I started. I even tried two applications one time and STILL had spiral left, so I just went back to the BSP... one app, sand, done.

                I usually just wipe/daub the stuff on with a bare finger (probably not the brightest idea, but oh well, SOMETHING's gonna kill me sooner or later anyway) and it's quick and easy. Only downside is you get the "funky pink finger" LOL

                later! OL JR
                I put on a glove. Now if only I would remember to put on a dust mask when I'm sanding. I'm not sure why you got those results with CWF; it works for me. Bondo putty turns the entire tube pink (due to dust adhesion) but that doesn't cause any problems. I will say that spirals filled with Bondo putty really stand out after sanding, because the putty remaining in them is a dark red. With CWF, they can be hard to see because the filler is a very light yellow in color. I have had great results with both, and I've also gotten less than complete filling in spots with both products. They are very different products but they produce essentially the same results, at least for the applications that I use them.
                Mark S. Kulka NAR #86134 L1,_ASTRE #471_Adirondack Mountains, NY
                Opinions Unfettered by Logic • Advice Unsullied by Erudition • Rocketry Without Pity
                +09281962-TAK-08272007+
                SAM # 0011

                Comment

                • luke strawwalker
                  BAR
                  • Dec 2007
                  • 6151
                  • Needville and Shiner, TX

                  #38
                  Originally posted by Mark II
                  I put on a glove. Now if only I would remember to put on a dust mask when I'm sanding. I'm not sure why you got those results with CWF; it works for me. Bondo putty turns the entire tube pink (due to dust adhesion) but that doesn't cause any problems. I will say that spirals filled with Bondo putty really stand out after sanding, because the putty remaining in them is a dark red. With CWF, they can be hard to see because the filler is a very light yellow in color. I have had great results with both, and I've also gotten less than complete filling in spots with both products. They are very different products but they produce essentially the same results, at least for the applications that I use them.
                  How does the CWF work for you on tube spirals?? I've had dismal luck with it... I've tried brushing on the thinned CWF that I use on nosecones and stuff, about the consistency of hot dog mustard, and I've tried daubing the stuff straight out of the can into the spiral, putting on a thick coat in a bead, etc... It can look good when you start, but as soon as I get the stuff sanded off down to the tube surface, the stuff in the spiral seems to be gone as well and the spiral looks just as present as it was when I started.

                  Now, the Bondo Spot Putty, I can daub that on over the spiral, let it dry, sand it down, and get a distinctive red line where the spiral was, true enough, but the thing is actually filled in... if you lightly run a fingernail down the length of the tube, it will hang on the CWF "filled" spiral, but won't on the BSP filled spiral-- so the material is still there, obviously. I'm wondering if the adhesion of the CWF is just too low for this application, and it all "turns loose" during sanding and "goes away", where the BSP does not-- it's strong enough in adherence to 'stay put' in the spiral and get sanded down flush with the surface of the glassine tube coating. That's my theory anyway...

                  I don't always fill the spiral-- kinda depends on the tube, and how noticeable it is, and just "how good" of a finish I want for the rocket. Sport fliers aren't as critical as say semi-scale models, obviously...

                  Just wondering... OL JR
                  The X-87B Cruise Basselope-- THE Ultimate Weapon in the arsenal of Homeland Security and only $52 million per round!

                  Comment

                  • hcmbanjo
                    When Pigs Fly!
                    • Sep 2005
                    • 1135
                    • Orlando, FL

                    #39
                    I'm going to have to try the Bondo Spot Putty. I'm always looking for the next best thing.
                    One thing I didn't notice in the responses - are some modeler's using too rough a sandpaper to sand down CWF in body tube seams? 400 grit is my choice for this.

                    For filling body tube seams, my end results have gotten better lately using a technique suggested by Bradycros on TRF.

                    After adding some CWF fin fillets he would cover the fillet area with CA.
                    This would "lock" the CWF down with less chance of it cracking and "flaking" out.

                    I agree with most here, I use very little CWF on the body tube seams, meaning I don't paint over the entire body tube.
                    I'll sand over the dried seam CWF not quite down to the surface. Picture the CWF in the seams as a capital "T" with a flattened (sanded down) top.
                    I'll then apply CA using a Q-Tip down the seam spiral top of the "T".
                    This CA cover will help lock the CWF in the seam. The CWF is water based and porous, the CA will penetrate it and into the body tube.

                    Then sand the top of the "T" down level with the body tube.

                    This has pretty much eliminated the CWF being sanded and knocked out of the seams.

                    Did you ever notice how well CWF stays in the seams when smoothing out a launch lug?
                    Hans "Chris" Michielssen
                    Old/New NAR # 19086 SR

                    www.oddlrockets.com
                    www.modelrocketbuilding.blogspot.com
                    http://www.nar.org/educational-resou...ng-techniques/
                    Your results may vary
                    "Nose cones roll, be careful with that."
                    Every spaceman needs a ray gun.
                    Look out - I'm the Meister Shyster!

                    Comment

                    • luke strawwalker
                      BAR
                      • Dec 2007
                      • 6151
                      • Needville and Shiner, TX

                      #40
                      Originally posted by hcmbanjo
                      I'm going to have to try the Bondo Spot Putty. I'm always looking for the next best thing.
                      One thing I didn't notice in the responses - are some modeler's using too rough a sandpaper to sand down CWF in body tube seams? 400 grit is my choice for this.

                      For filling body tube seams, my end results have gotten better lately using a technique suggested by Bradycros on TRF.

                      After adding some CWF fin fillets he would cover the fillet area with CA.
                      This would "lock" the CWF down with less chance of it cracking and "flaking" out.

                      I agree with most here, I use very little CWF on the body tube seams, meaning I don't paint over the entire body tube.
                      I'll sand over the dried seam CWF not quite down to the surface. Picture the CWF in the seams as a capital "T" with a flattened (sanded down) top.
                      I'll then apply CA using a Q-Tip down the seam spiral top of the "T".
                      This CA cover will help lock the CWF in the seam. The CWF is water based and porous, the CA will penetrate it and into the body tube.

                      Then sand the top of the "T" down level with the body tube.

                      This has pretty much eliminated the CWF being sanded and knocked out of the seams.

                      Did you ever notice how well CWF stays in the seams when smoothing out a launch lug?
                      I use either 220 or 400 grit to sand the spirals... don't recall which ATM...

                      Later! OL JR
                      The X-87B Cruise Basselope-- THE Ultimate Weapon in the arsenal of Homeland Security and only $52 million per round!

                      Comment

                      • jetlag
                        Old BAR
                        • Aug 2006
                        • 2294

                        #41
                        Hans,

                        CWF for fillets adds very little for strength, which is what I always thought the purpose of fillets was...Strength.
                        I don't go to TRF, so I have not read over that particular thread; if aesthetics are your only concern, then by all means keep making fillets with CWF. However, if strength is what you are after, that is the wrong stuff.
                        I use epoxy, which some here think is overkill. That's OK, too! At least I never have fins that flatten out with heat. Ever.

                        Allen

                        Comment

                        • jeffyjeep
                          Old Submariner
                          • Jan 2009
                          • 8465
                          • Home of Wayne & Garth

                          #42
                          Same here. I use epoxy------ONLY. I'd rather have overkill than underkill (or whatever the opposite is of overkill.......................................... ......................overreanimate? overletlive?)
                          Never trust an atom. They make up everything.

                          4 out of 3 people struggle with math.

                          Chemically, alcohol IS a solution.

                          NAR# 94042
                          SAM# 0078

                          Comment

                          • hcmbanjo
                            When Pigs Fly!
                            • Sep 2005
                            • 1135
                            • Orlando, FL

                            #43
                            Sorry, I should have been more specific.
                            On LPR rockets: After gluing the fins in place, I use white glue for fillets.
                            I've used CWF afterwards and over white glue fillets when I wanted to build up the fillet area. CWF by itself would be too weak for a fillet.
                            I'm not suggesting it alone for a fin fillet.

                            I have used epoxy fillets on larger models.
                            Hans "Chris" Michielssen
                            Old/New NAR # 19086 SR

                            www.oddlrockets.com
                            www.modelrocketbuilding.blogspot.com
                            http://www.nar.org/educational-resou...ng-techniques/
                            Your results may vary
                            "Nose cones roll, be careful with that."
                            Every spaceman needs a ray gun.
                            Look out - I'm the Meister Shyster!

                            Comment

                            • Solomoriah
                              Incorrigible Kit Basher
                              • Jul 2006
                              • 1940
                              • USA

                              #44
                              I almost never use epoxy on fins... but then, I have a fully upright storage arrangement, so I've never had a problem with sagging fins. I did use epoxy fillets on my BT-70 3x18 Ultimatum but I didn't on my 4x18 Big Daddy. But then, the Big Daddy is through-the-wall, and sagging seems vanishingly unlikely for it.

                              I do sometimes use FnF/CWF after filleting with glue, mainly to fill in any bubbles or dings that may remain. Generally only when I've hand-cut the fins.
                              NAR # 115523
                              Once upon a better day... SAM #0076
                              My site: http://rocketry.gonnerman.org

                              Comment

                              • jetlag
                                Old BAR
                                • Aug 2006
                                • 2294

                                #45
                                If you used epoxy in the first place, you'd never have to go back over the white glue to fill air bubbles. Why make a one step job two? The weight increase is minimal compared to the increase in overall strength.
                                Epoxy makes beautiful fillets and cleans up with a little alcohol. I never use a glove!